| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded |
| Manufacturer | Aclo Compounders |
| Trade Name | Accucomp |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Accucomp ABS ABS801L Medium Impact Grade.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | MD; ASTM D955 |
| Melt Flow | 2.0 g/10 min | 2.0 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 102 | 102 | ASTM D785 |
| Tensile Strength at Break | 35.0 MPa | 5080 psi | ASTM D638 |
| Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 |
| Elongation at Break | 14 % | 14 % | ASTM D638 |
| Elongation at Yield | 3.0 % | 3.0 % | ASTM D638 |
| Tensile Modulus | 1.900 GPa | 275.5 ksi | ASTM D638 |
| Flexural Strength | 63.0 MPa | 9140 psi | ASTM D790 |
| Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
| Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 83.9 °C | 183 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | |
| Flammability, UL94 | HB <br>@Thickness 1.59 mm |
HB <br>@Thickness 0.0625 in |
UL File #E56070 |