| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded | 
| Manufacturer | Flint Hills Resources | 
| Trade Name | |
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Flint Hills H0500HN Polypropylene Homopolymer.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 | 
| Melt Flow | 5.0 g/10 min | 5.0 g/10 min | ASTM D1238 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Rockwell R | 111 | 111 | ASTM D785 | 
| Tensile Strength, Yield | 37.0 MPa | 5370 psi | ASTM D638 | 
| Elongation at Yield | 7.7 % | 7.7 % | ASTM D638 | 
| Flexural Modulus, 1% Secant | 1560 MPa | 226000 psi | ASTM D790 | 
| Izod Impact, Notched |           0.400           J/cm           @Temperature 23.0 °C  | 
                  0.749           ft-lb/in           @Temperature 73.4 °F  | 
        ASTM D256 | 
| Gardner Impact |           6.00           J           @Temperature 23.0 °C  | 
                  4.43           ft-lb           @Temperature 73.4 °F  | 
        ASTM D5420 | 
| Tangent Modulus | 1650 MPa | 239000 psi | ASTM D790 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 241 °F | ASTM D648 | 
| Flammability, UL94 | HB | HB |