Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IRPC Polimaxx Polene 1102H Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene 1102H Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CHARACTERISTICS: GOOD STIFFNESS, GOOD EXTRUDABILITY, HIGH IMPACTAPPLICATIONS: MONOFILAMENT/YARN/SHEET EXTRUSION FOR THERMOFORMINGBLOW MOLDING AND INJECTION MOLDING FOR ROPESCOARSE TEXTILE FOR JUMBO BAGSINDUSTRIAL CONTAINERSSTRETCH TAPECORRUGATE SHEETBOTTLESCLOSURESSHEETS FOR FILESHEET EXTRUSION FOR THERMOFORMING CUPS AND DAIRY CONTAINERS
Physical Properties Metric English Comments
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Yield 37.0 MPa
5370 psi
ASTM D638
Elongation at Yield 28 %
28 %
ASTM D638
Flexural Modulus 1.60 GPa
232 ksi
1% Secant; ASTM D790
Charpy Impact, Notched 0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Heat Distortion Temperature 110 °C
230 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 170 - 290 °C
338 - 554 °F