Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM D638 |
Nylene® PA6/6 Glass/Mineral Filled 7215 HS Nylon 6/6 15% Glass Reinforced/25% Mineral Filled.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Tensile Strength, Yield | 130 - 150 MPa | 18900 - 21800 psi | Average value: 141 MPa Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ISO 527, ASTM D638 |
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha.. |
|||
Tensile Strength, Yield | 130 - 210 MPa | 18900 - 30500 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 130 - 280 MPa | 18900 - 40600 psi | |
Materion Beryllium Copper Alloy 25 Forgings & Extrusions; A (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 130 - 210 MPa | 18900 - 30500 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 130 - 250 MPa | 18900 - 36300 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 130 MPa @Strain 0.200 %, Temperature 980 °C |
18900 psi @Strain 0.200 %, Temperature 1800 °F |
|
Haynes 25 alloy, hot rolled and 1230°C solution annealed sheet Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 130 - 210 MPa | 18900 - 30500 psi | |
Materion Beryllium Copper Alloy M25 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX04489C PC LNP STAT-KON* DX04489C is a high modulus compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Con.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East) VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light.. |
|||
Tensile Strength, Yield | 130 MPa @Temperature 550 °C |
18900 psi @Temperature 1020 °F |
Annealed prior to test |
Special Metals INCOLOY® Alloy 800HT™ A nickel-iron-chromium alloy having the same basic composition as INCOLOY alloy 800 but with significantly higher creep-rupture strength. The higher strength results from close control of the carbo.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM-D638 |
Polyram PlusTek PA301G3 Nylon 6.6, Heat Stabilized, 15% Glass Fiber Heat stabilized, 15% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM-D638 |
Polyram PlusTek RD302G6 Nylon 12, 30% Glass Fiber 30% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM-D638 |
Polyram RamSter PF300G6 PBT, 30% Glass Fiber 30% Glass-Fiber reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ISO 527 |
Polyram RamSter PF305G6 PBT, 30% Glass Fiber 30% Glass fiber reinforced, PBT for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM-D638 |
Polyram RamTough PZ300G6 Polycarbonate, 30% Glass Fiber 30% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ISO 527 |
Polyram RamLloy PFS301G6 ASA/PBT Alloy, 30% Glass Fiber 30% Glass fiber reinforced ASA/PBT alloy for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM D638, ISO R527 |
EPICHEM Epiter PBT GF 30 Polybutylene Terephthalate, 30% Glass Characteristics: 30% glass fibre filled |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM D638 |
E-Polymers TEKAMID® TA250G15 , 15% Glass Fiber Reinforced PA66, DAM 15% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM D638 |
E-Polymers TEKANATE™ G715FR , Flame Retardant, 15% Glass Fiber Reinforced Poly Carbonate 15% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 130 MPa @Strain 0.200 % |
18900 psi @Strain 0.200 % |
|
ALIMEX ACP 5080 Aluminum Cast Plate ACP 5080 is a 5xxx series precision aluminum cast plate. Thickness, flatness and surface finish offer very tight tolerances.Material stability and excellent processing characteristics make this alum.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry) Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® A3X4G7 35% Glass Filled PA66 FR (Dry) Description: 35% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stiffness and stre.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ASTM D638 |
Cheng Yu Plastic A707G2 SAN, 20% Glass Fiber |
|||
Tensile Strength, Yield | 130 MPa @Strain 0.200 % |
18900 psi @Strain 0.200 % |
|
ALIMEX ACP 5080R Aluminum Cast Material Sizes range availability along with good mechanical and physical properties of ACP 5080R provide the Mold Tool Industry tooling materials solutions for the most challenging applications.Information .. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, Conditioned Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East) VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |
|||
Tensile Strength, Yield | 130 MPa | 18900 psi | ISO 527 |
Polyram PlusTek RA320G5 Nylon 66 for Injection Molding, 25% Glass-Fiber Reinforced, Flame Retardant and High Stiffness 25% Glass-fiber reinforced, flame retardant and high stiffness Nylon 66 for injection molding applications.Information provided by Polyram. |