Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Materion Beryllium Copper Alloy M25 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17300)

Category Metal , Nonferrous Metal , Beryllium Alloy , Copper Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion Beryllium Copper Alloy M25 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17300).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.36 g/cc
0.302 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 400 - 540 MPa
58000 - 78300 psi
Tensile Strength, Yield 130 - 210 MPa
18900 - 30500 psi
Elongation at Break 30 - 60 %
30 - 60 %
Modulus of Elasticity 131 GPa
19000 ksi
Machinability 60 %
60 %
Thermal Properties Metric English Comments
CTE, linear 17.0 µm/m-°C

@Temperature 20.0 - 200 °C
9.44 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 105 W/m-K
729 BTU-in/hr-ft²-°F
Melting Point 870 - 980 °C
1600 - 1800 °F
Solidus 870 °C
1600 °F
Liquidus 980 °C
1800 °F
Component Elements Properties Metric English Comments
Beryllium, Be 1.8 - 2.0 %
1.8 - 2.0 %
Co + Ni >= 0.20 %
>= 0.20 %
Co + Ni + Fe <= 0.60 %
<= 0.60 %
Copper, Cu 97.5 %
97.5 %
as balance
Lead, Pb 0.20 - 0.60 %
0.20 - 0.60 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000910 - 0.0000115 ohm-cm
0.00000910 - 0.0000115 ohm-cm
15-19% IACS Conductivity