Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 115 MPa | 16700 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM UH1026 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ISO 527 |
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet) KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re.. |
|||
Tensile Strength, Yield | 115 MPa @Temperature 23.0 °C |
16700 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ASTM D638 |
Radici Radilon® N66-SRV130 Nylon 66
(discontinued **) |
|||
Tensile Strength, Yield | >= 115 MPa | >= 16700 psi | |
MetalTek MTEK 20% Ni 412 Cast UNS C97600 Nickel-Silver Information provided by MetalTekCast UNS C97600; Cast Grade C97600; Cast ASTM B271, B584; Military MIL-C-17112 |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ISO 527 type 1 A |
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in.. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1285 PEI (Europe-Africa-Middle East) Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ASTM D638 |
Solvay Specialty Polymers PrimoSpire® PR-351 Polyphenylene, Self-Reinforced (SRP) PrimoSpire® PR-351 resin is a higher flow, injection molding grade of PrimoSpire® self-reinforced polyphenylene (SRP). PrimoSpire® SRP resin is an ultra-high performance amorphous, melt-pro.. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ASTM D638 |
Techmer ES HiFill FR® PBT GF30 FR 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ASTM D638 |
SPS Guang Zhou PONYLâ„¢ EP4003G20 Non-halogen flame retardance/GF20%-PA66 Characteristic: Good flame retardance, high mechanical properties, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer LNP* THERMOCOMP* KF006XXC is a compound based on Acetal Copolymer resin containing 30% Glass Fiber. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer (Asia Pacific) LNP* Thermocomp* KF006XXC is a compound based on Acetal Copolymer resin containing Glass Fiber. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF003ES PA 66 LNP* THERMOCOMP* RF003ES is a Nylon 66 base resin containing 15% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | D638 |
Zhejiang Juner 201-G30 30% Glass Fibre Reinforced Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ISO 527 |
Polyram PlusTek PD502G6 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced 30% Glass-fiber reinforced, V-0 1.6 mm, Nylon 12 for injection molding application.Information provided by Polyram. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-30 EC PA6-GF30 Information provided by EMS Grivory |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ISO 527 |
Eurostar Staramide RFM3353EM PA66/6, Glass/Mineral Fiber Reinforced, Injection Molding Starflam RFM3353EM is a Mineral Filled, Glass Fiber Reinforced Polyamide 66/ Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | 50mm/min; ISO 527 |
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Conditioned) Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ASTM D638 |
Beijing Ranger Chem PBT 403 M-G20 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | 50mm/min; ISO 527 |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Conditioned) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | 50 mm/min; Same value from ASTM and ISO test. |
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he.. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD4413 PC (Europe-Africa-Middle East) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC (Asia Pacific) LNP* Lubricomp* DFL369XF is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ISO 527 |
Polyram PlusTek RA325G4 Nylon 66 for Injection Molding, 20% Glass-Fiber Reinforced, Self-Extinguishing, Halogen Free 20% Glass-fiber reinforced, self-extinguishing halogen free Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ISO 527 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |
|||
Tensile Strength, Yield | 115 MPa | 16700 psi | ASTM D638 |
Techmer ES HiFill FR® PBT GF30 FR X 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame RetardantUL File Number: E157318TPCI# 1006011Information provided by TP Composites, In.. |