Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ASTM D638 |
Ovation Polymers Opnyl OP66GF15 Nylon 66, 14% Glass Reinforced Nylon 66 - Glass reinforced (14 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Faradex ES003DE PEI LNP* Faradex* ES003DE is a Polyetherimide resin containing stainless steel fibers. Characteristics of this grade are EMI/RFI Shielding.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 105 MPa @Temperature 23.0 °C |
15200 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 90G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Tensile Strength, Yield | 105 - 234 MPa | 15200 - 34000 psi | Average value: 180 MPa Grade Count:55 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ISO 527 |
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1000F PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be sup.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1000FV PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010KM PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010KM PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1100EF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1100V PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 2412EPR PEI 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 9011 PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM MD141 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON ZE0039 PPO LNP* STAT-KON* ZE0039 is a compound based on PPO resin containing 15% Carbon Fiber. Added features of this grade includes: Flame Retardant, Electrically Conductive. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC (Asia Pacific) 20% Glass Fiber Reinforced Polycarbonate. Some light color grades may have lower impact data than nature and black grade. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM AUT200 PEI Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperat.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ASTM D638 |
Westlake Plastics Tempalux® Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ASTM D638 |
Westlake Plastics Tempalux® Polyetherimide For Medical Applications Medical grade Tempalux is made from Ultem® polyetherimide resin, an amorphous thermoplastic which exhibits excellent resistance to a wide range of chemicals and disinfectants. Ultem maintains its .. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ASTM D638 |
E-Polymers Tekaloy® G70GR , 30% Glass Reinforced PC/ABS Alloy 30% Glass Fiber reinforced, High stiffness, Dimensional stabilityInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527-2 |
BASF Ultradur® FRee B 4450 G5 LS 25% Glass Filled PBT Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ASTM-D638 |
Polyram PlusTek RA320G3 Nylon 6.6, 15% Glass Fiber, Flame Retardant 15% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |