Mechanical Properties Metric English Comments
Tensile Strength, Yield 91.0 MPa
13200 psi
50 mm/min; ISO 527
SABIC Innovative Plastics LNP COLORCOMP J1000 PES (Europe-Africa-Middle East)
LNP* COLORCOMP* J1000 is a compound based on Polyethersulfone resin.
Tensile Strength, Yield 91.0 MPa
13200 psi
50 mm/min; ISO 527
SABIC Innovative Plastics LNP COLORCOMP J1000E PES (Europe-Africa-Middle East)
LNP* COLORCOMP* J1000E is a compound based on PES resin. Added features include: Easy Moulding.
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC
LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing 30% Mixed Glass, 15% PTFE. Added features of this material include: Internally Lubricated.
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Gharda Chemicals GATONE™ 5700 Polyetheretherketone (PEEK)  (discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
Tensile Strength, Yield 91.0 MPa
13200 psi
ISO 527-2/1A/50
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula..
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Gharda Chemicals Gafone™ 3100 Polyethersulfone (PES)  (discontinued **)
Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl..
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica..
Tensile Strength, Yield 90.7 MPa

@Thickness 3.20 mm
13200 psi

@Thickness 0.126 in
5mm/min; ASTM D638
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Tensile Strength, Yield 91.03 MPa
13200 psi
ASTM D638
Lucent Polymers GPCB-110 Polycarbonate+PBT, 10% Glass Fiber Reinforced
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Tensile Strength, Yield 91.03 MPa
13200 psi
ASTM D638
Lucent Polymers GPCB-330 Polycarbonate+PBT, 30% Glass Fiber Reinforced, Impact Resistant
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Tensile Strength, Yield 91.0 MPa

@Strain 0.200 %,
Temperature 980 °C
13200 psi

@Strain 0.200 %,
Temperature 1800 °F
Haynes Hastelloy® X alloy, sheet
Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ..
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Techmer ES Elastoblend® PA6/6 GF13 IM HS L 13% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact Modifi..
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Techmer ES Elastoblend® PA6/6 GF13 IM-1 HS L 13% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri..
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Techmer ES Elastoblend® PA6/6 GF13 IM2 BK 13% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri..
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Techmer ES Elastoblend® PA6/6 GF14 IM HS L BK 14% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri..
Tensile Strength, Yield 91.0 MPa
13200 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP ZFL34 PPE+PS
LNP* LUBRICOMP* ZFL34 is a compound based on PPE+PS resin containing 20% Glass Fiber, 15% PTFE. Added feature of this gradae is: Wear Resistant.
Tensile Strength, Yield 91.0 MPa
13200 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp ZFL34 PPO
LNP* Lubricomp* ZFL34 is a compound based on Modified PPO containing glass fiber and PTFE.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength, Yield 91.0 MPa
13200 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON RFD03 PA 66
LNP* STAT-KON* RFD03 is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material is: Electrically Conductive.
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Techmer ES HiFill® PET GF/M35 35% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightInformation provided by TP Composites, Inc.
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Techmer ES Luriblend® HTN 01420 BK
Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: Good Wear Resistance, Low Friction, High Heat Resistance and LubricatedAppearance: BlackInformation provide..
Tensile Strength, Yield 91.0 MPa
13200 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP EX00781H PEI
LNP* THERMOCOMP* EX00781H is a compoud based on Polyetherimide containng Proprietary Filler(s). Added feature of this material is: Healthcare.
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU
LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing 20% Glass Fiber.
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Techmer ES HiFill® PA6/6 WM40 IM HS 40% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessin..
Tensile Strength, Yield 91.0 MPa
13200 psi
dry; ISO 527
Ter Hell Plastic Terez® PA 6 7751 TGF 15 GL Polyamide 6, 15% Glass Fiber
Description: Medium viscosity, dry impact resistant PA 6, 15% glass fiber reinforced and improved surface gloss.Application: For molding parts with good stiffness and high dimensional stability.In..
Tensile Strength, Yield 91.0 MPa
13200 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info..
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Aclo Accutech SAN SAN930G20L Glass Reinforced
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific)
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated.
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM 638
PlastxWorld CEVIAN® B2504 20% GF PBT/ABS Alloy
Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc.
Tensile Strength, Yield 91.0 - 145 MPa
13200 - 21000 psi
Average value: 114 MPa Grade Count:4
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU (Asia Pacific)
LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing Glass Fiber.