Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 23°C; 50% RH; ASTM D638 |
PTS Lucet® GC-225 25% Glass Reinforced Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 98.1 MPa @Thickness 3.20 mm |
14200 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity Feature: Injection Molding, POM+GF10%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 98.1 MPa @Thickness 3.20 mm |
14200 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUCON PO6063 mPPO+CNT+CF+GF Description: Injection Molding, mPPO+CNT+CF+GF, Electrostatic Dissipation, High Strength, Low WarpageApplication: LCD Cell TrayCAS No. 35134-01-4, 65997-17-3, 7440-44-0 and 7782-42-5Information prov.. |
|||
Tensile Strength, Yield | 98.1 MPa @Thickness 3.20 mm |
14200 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOS GP2205 SAN+GF20%, General Purpose Feature: Injection Molding, SAN+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 98.1 MPa @Thickness 3.20 mm |
14200 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b.. |
|||
Tensile Strength, Yield | 98.1 MPa @Thickness 3.20 mm |
14200 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance Description: Injection Molding, PC+GF20%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® CF-3200HF PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® EM-8240C MPPE, Glass Filled MPPE/GF material that is used in the main frame of banknote sortersInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® EM-8250G MPPE, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-5150GT PBT, 15% Glass Filled Low warpage with 15% GF reinforcement and can be used in the switches for microwave or ovensInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® LS-3302A PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® TK-6036H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® CF-3200HF PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® EM-8240C MPPE, Glass Filled MPPE/GF material that is used in the main frame of banknote sortersInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® EM-8250G MPPE, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-5150GT PBT, 15% Glass Filled Low warpage with 15% GF reinforcement and can be used in the switches for microwave or ovensInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | ASTM D638 |
Samyang Tribit® 1500G15 Polybutylene Terephthalate, 15% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® LS-3302A PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® TK-6036H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | ASTM D638 |
Cheng Yu Plastic ML3420 PC, 20% Glass Fiber |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | ASTM D638 |
Cheng Yu Plastic NG1100S Nylon 66, 10% Glass Fiber Reinforced |
|||
Tensile Strength, Yield | 98.1 MPa | 14200 psi | ASTM D638 |
Cheng Yu Plastic FR200GV10 Flame Retardant Nylon 66, 10% Glass Fiber |
|||
Tensile Strength, Yield | 98.1 - 216 MPa | 14200 - 31300 psi | Average value: 145 MPa Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are .. |
|||
Tensile Strength, Yield | 98.1 MPa @Thickness 3.20 mm |
14200 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUCON CP6067 PC+CNT+CF Description: Injection Molding, PC+CNT+CF, Electrostatic Dissipation, High Strength, High Flow & Good ProcessabilityApplication: Wafer Carrier Box, Conveyor belt bearing blockCAS No. 103598-77-2, 74.. |