Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP PX99848 PA 6 LNP* COLORCOMP* PX99848 is an unfilled Nylon 6 resin. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP PX99848 PA 6 (Asia Pacific) LNP* Colorcomp* PX99848 is a compound based on Nylon 6 resin containing Unfilled Custom Color. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® 12-032
(discontinued **) PRE-ELEC 12-032 is a conductive thermoplastic compound based on a polyacetal copolymer with 20% carbon fiber. PRE-ELEC 12-032 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 50 mm/min |
Arkema Group Oroglas® MI-4T Acrylic, Heat Resistant
(discontinued **) OROGLAS MI-4T is an acrylic grade that associates improved impact resistance with high heat resistance.Key features improved impact resistance: up to 4 times more impact resistant than standard acr.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Tensile Strength, Yield | 76.0 MPa @Strain 0.200 %, Temperature 1095 °C |
11000 psi @Strain 0.200 %, Temperature 2003 °F |
|
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX9406P PPE NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific) LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 2 in/min; ASTM Test |
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry) Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ISO 527 |
Polyram PlusTek PA340S4 Nylon 66 for Injection Molding, 20% Glass-Beads Reinforced 20% Glass-beads reinforced Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | D638 |
Zhejiang Juner 301-G10 10% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | |
Covestro Makroblend® UT-620 G Polycarbonate + Polyester Blend Key Features:Contains FillerHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 Septembe.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
Diamond Polymers NYLON 6 Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM Data |
Dow Tyril® 880B SAN TYRIL® 880B SAN copolymer combines the high levels of chemical resistance, heat resistance and overall strength of 880 resin with improved mold flow and mold release characteristics.Data provided b.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM Data |
Dow Tyril® 880 SAN TYRIL® 880 SAN copolymer offers excellent physical properties incorporating the highest levels of chemical resistance, heat resistance and overall strength of any TYRIL grade.Data provided by Dow C.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 GF2 POM 10% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | v = 50 mm/min; ISO 527-2 |
CENTROPLAST CENTROMID 6 E Polyamide 6 extruded This tough and impact resistant material has good chemical resistance and can be bonded and welded. It is used for sealing rings, flanges, etc. Information provided by CENTROPLAST Engineering Plast.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
Ashley Polymers Ashlene® 149WO PBT Polyester, 45% Glass Reinforced A flame retardant PBT polyester with 45% glass reinforcement, mineral filled.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | v = 50 mm/min; ISO 527-2 |
CENTROPLAST CENTROMID 6 E FG Polyamide 6 extruded, Food Grade This tough and impact resistant material has good chemical resistance and can be bonded and welded. Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | dry; ISO 527-1/-2 |
Murtfeldt Murylat® SP Polyethylene Terephthalate Murylat® SP combines the properties of Murylat® with improved wear and friction characteristics. It also has increased dynamic resilience which, for example, significantly reduces the required dri.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ISO value at 50 mm/min. |
BASF Capron® 8362 HS Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8362 HS is a 34% glass reinforced, impact modified, heat stabilized nylon6 injection molding compound exhibiting a high level of toughness in combination with excellent processability and sur.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ISO value at 50 mm/min. |
BASF Capron® 8362 HS BK-102 Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8362 HS BK-102 is a pigmented black, 34% mineral reinforced, impact modified, heat stabilized nylon 6 injection molding compound exhibiting a high level toughness in combination with excellen.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp TX88477 PU LNP* Thermocomp* TX88447 is a compound based on Polyurethane resin containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
Custom Resins Norpex® 300 PPE (Polyphenylene Ether)
(discontinued **) Premium performance high heat. Properties for dry as molded samples.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | v = 50 mm/min; ISO 527-2 |
CENTROPLAST CENTRO HPM Polyphenylensulfone This plastic has very good mechanical, electrical and thermal properties. It has very good hydrolysis resistance, and is suitable for medical, and pharmaceutical equipment construction.Information .. |