Mechanical Properties Metric English Comments
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Omni Plastics OmniTech™ HDPE GRC30 Glass Reinforced
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
Tensile Strength, Yield 68.9 MPa
10000 psi
2 in per min; ASTM D638
Network Polymers MS 600 Styrene Methyl Methacrylate Copolymer
Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Polymer Resources PPX-G10HF Modified-PPO, 10% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Tensile Strength, Yield 68.9 - 150 MPa
10000 - 21800 psi
Average value: 106 MPa Grade Count:37
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Tensile Strength, Yield 68.9 MPa
9990 psi
ASTM D882
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant
Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i..
Tensile Strength, Yield 68.9 MPa
10000 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
PolyOne Stat-Tech™ AS-15NCF/000 ABS - 15% Nickel Coated Carbon Fiber  (discontinued **)
Data provided by PolyOne.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Fiberfil® J-60/20/E Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Fiberfil® J-60/20/E4 Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Fiberfil® J-60/20/H Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Techmer ES HiFill® ECTFE GF25 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightFeatures: CopolymerAppearance: Natural ColorInformation provided by TP Composites, Inc.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Techmer ES HiFill® HIPS GF20 BK 20% Glass Filled
Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Spartech PP5420 Glass Fiber Reinforced Homopolymer
Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Techmer ES HiFill® PA6 GB20 L 20% Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Techmer ES HiFill® PEEK HF
Availability: North AmericaForms: PelletsFeatures: Low ViscosityInformation provided by TP Composites, Inc.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Techmer ES HiFill® PP GF20 CC LE 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically Coupled and Low ExtractablesInformation provided by TP Composites, ..
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Techmer ES Plastiblend® PA6/6 HS L N Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and Nucleating AgentFeatures: Heat Stabilized, Impact Modified and NucleatedProcessing Method: Injection MoldingIn..
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Techmer ES Plastiblend® PA6/6,6 IM 3757 Nylon 6/66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedProcessing Method: Injection Mold..
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM 638
PlastxWorld CEVIAN® SERG1 10% GF ABS
Glass fiber reinforced and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Westlake Plastics Ardel® Polyarylate
Stock shapes extruded from Ardel resin are specifically formulated to endure the damaging effects of UV light. When exposed to UV light, this unique material undergoes a molecular rearrangement res..
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin
NSF Standard 61 CertifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Tensile Strength, Yield 68.9 MPa
9990 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers SAN 330 BEADS Styrene Acrylonitrile, Transparent Engineering Thermoplastic, High Flow Natural Beads
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Clariant PCSP0014 GREY Polycarbonate, Stainless Steel Fiber, EMI
Data provided by Clariant Masterbatches
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Clariant Renol PC010-L FR Polycarbonate, Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6)
Tecast® 6PA Black is a black cast nylon that is more UV resistant than natural nylon 6.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combina..
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Clariant Renol 6602-L Nylon 66, Internally Lubricated
Data provided by Clariant Masterbatches
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Asahi Kasei Thermylene® P6-20FG-0600 20% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Asahi Kasei Thermylene® P6-20FG-0659 20% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
PolyOne Edgetek® UR-20GF/000 Natural Thermoplastic Polyurethane (Ether-Based), 20% Glass Fiber Reinforced  (di
Information provided by PolyOne™ Corporation
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Spartech EP6430 Filled and Reinforced Copolymer
Filled copolymers offer a higher level of impact performance than homopolymer materials, and higher stiffness than unfilled copolymers. Copolymer based materials retain much of their impact strength..