Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 10000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 69.0 MPa
10000 psi
ASTM D638
Nylene® Norpex® AX290 PPE (Polyphenylene Ether); High Performance High Heat
Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Tensile Strength, Yield 69.0 MPa
10000 psi
ASTM D638
Nylene® PA6/6 Mineral Filled 6440 HS Nylon 6/6
34% Mineral Filler; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Tensile Strength, Yield 69.0 MPa
10000 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics Cycolac® INP563 ABS
SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Tensile Strength, Yield 69.0 MPa
10000 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha..
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Polymer Resources TPSF-FRG10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, ..
Tensile Strength, Yield 68.9 MPa
10000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® GF 5209 10 FPS 15 BLACK 30 A 1 Acetal-Copolymer, Glass Filled  (discontinued **)
PRELIMINARY DATA SHEETDescription/Features:Glass Fiber ReinforcedBlackInformation provided by PolyOne Corporation.
Tensile Strength, Yield 69.0 MPa
10000 psi
ASTM D638
Global POM-100 High Viscosity Acetal Homopolymer
Information provided by Global Polymers Corporation.
Tensile Strength, Yield 68.9 MPa
10000 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® ACR100 Polymethylmethacrylate
High heat injection molding grade of PMMAAll information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 69.0 MPa
10000 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DD0009XP PC
LNP* STAT-KON* D-FR is a compound based on Polycarbonate resin containing Carbon. Added features of this grade include: Flame Retardant, Electrically Conductive.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Techmer ES HiFill® ECTFE GF25 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightFeatures: CopolymerAppearance: Natural ColorInformation provided by TP Composites, Inc.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Techmer ES HiFill® PA4/6 GF5 HS BK002 5% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackInformation provided b..
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Techmer ES Luriblend® PA6/6 X Nylon 66
Availability: North AmericaForms: PelletsAdditive: Lubricant Features: Lubricated, Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc.
Tensile Strength, Yield 69.0 MPa
10000 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific)
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
Tensile Strength, Yield 68.9 MPa

@Thickness 3.17 mm
10000 psi

@Thickness 0.125 in
Type I; ASTM D638
Sumitomo Chemical Sumipex® BF3 Acrylic Resin, GP Blow Molding Grade
Product CharacteristicsExcellent WeatherabilityHigh TransparencyGood Heat ResistanceInformation provided by Calsak Corporation
Tensile Strength, Yield 69.0 MPa
10000 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS
EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l..
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin
NSF Standard 61 CertifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Ensinger Tecamid® HS Nylon (PA)
Heat Stabilized nylon, increased ability to withstand the negative effects of heat exposure and increased overall service temperature over nylon 6/6.Information provided by Ensinger, Inc.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Ensinger Tecast™ 6PA Natural Unfilled Cast Nylon 6 (PA6)
Tecast® 6PA Natural is an FDA-compliant grade used in applications requiring cast nylon but without any fillers.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of..
Tensile Strength, Yield 69.0 MPa
10000 psi
ISO 527
Eurostar Star L PA66 D61 PA66, Injection Molded
Star L PA66 D51 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Tensile Strength, Yield 69.0 MPa
10000 psi
5 mm/min; ISO 527
Eurostar Starflam PX06012 PA6, Flame Retardant, Injection Molded
Starflam PX06012 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Clariant Renol 6602-L Nylon 66, Internally Lubricated
Data provided by Clariant Masterbatches
Tensile Strength, Yield 69.0 MPa
10000 psi
ASTM Data
Dow Tyril® 100 SAN
Data provided by Dow Chemical.
Tensile Strength, Yield 69.0 MPa
10000 psi
ASTM Data
Dow Tyril® 1000B SAN
TYRIL® 1000B SAN copolymer offers the best balance of physical properties of all TYRIL grades. It also provides excellent processability and chemical resistance, superior heat resistance, and good ..
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Asahi Kasei Thermylene® P6-20FG-1740 20% Glass Fiber Reinforced, High Impact
Information provided by Asahi Thermofil
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Asahi Kasei Thermylene® P1-20FG-2703 20% Glass Fiber Reinforced, Impact Modified
Information provided by Asahi Thermofil
Tensile Strength, Yield 68.97 MPa
10000 psi
ASTM D638
Lucent Polymers POM-500 Acetal Homopolymer, General Purpose, Injection Grade
Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Tensile Strength, Yield 69.0 MPa

@Temperature 23.0 °C
10000 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFE8200 BK431 is an unreinforced, toughened, heat stabilized, lubricated high performance polyamide resin for injection molding. It is also a PPA resin.Information provided by DuPont Perfo..
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Techmer ES Electrablend® PC SS15 15% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc.
Copyright © lookpolymers.com All Rights Reserved