Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 51.0 MPa | 7400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS Color Package may affect performance. Visual Fx PC+ABS in various metallic (Ares) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTWE280 ASA (Europe-Africa-Middle East) Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® ML7666 PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Asia Pacific) LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East) XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific) Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | ISO 527 |
FKuR Kunststoff Bio-Flex® S 9533 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Tensile Strength, Yield | 51.0 MPa @Thickness 3.20 mm |
7400 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY GP5006AF PC/ABS, Flame Retardant Description: Injection Molding, PC/ABS, Flame RetardantApplication: Electric and Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chem.. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp DP003XXP PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DP003XXP is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features include: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa.. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP NXCY620 PC+ABS LNP* LUBRICOMP* NXCY620 is a compound based on Cycoloy* XCY620 containing Silicone. Added feature of this material is: Lubricant. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Europe-Africa-Middle East) LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific) Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 325 PBT General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | ISO 527 |
Styrolution Novodur® H802 ABS Novodur H802 is a high heat injection molding grade with high stiffness, especially suitable for being painted.Information provided by Styrolution |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SF-0505EH MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 51.0 MPa @Thickness 3.17 mm |
7400 psi @Thickness 0.125 in |
ASTM D638 |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6 LNP* Thermocomp* PH0600B is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC.. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | ASTM Data |
Styron Pulse® 710 ABS + Polycarbonate PULSE® 710 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 710 Engineering resin h.. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | ASTM D638 |
Techmer ES Electrablend® PA12 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: /Glass/Stainless Steel FiberFeatures: ConductiveTPCI# 9873105Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | 50 mm/min |
Arkema Group Nakan® RPX 301 L PVC, Rigid Extrusion Grade NAKAN RPX 301 L is a rigid polyvinyl chloride compound developed for extrusion of transparent profiles for outdoor applications.ISO data provided by the manufacturer, Arkema. |
|||
Tensile Strength, Yield | 51.0 MPa @Thickness 3.20 mm |
7400 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron IPM2000 PMMA- ABS Alloy High Gloss, High scratch resistanceInformation provided by Bhansali |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp DBS 3602 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Good Impact Resistance Uses: Piping Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Tensile Strength, Yield | 51.0 MPa | 7400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |