Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 46.2 MPa | 6700 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M3500 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M5005 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ AT-000/10T Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Novablend™ 9562 Polyvinyl Chloride Alloy (PVC Alloy) Custom MoldingInformation provided by PolyOne |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D638 |
Ravago Manufacturing Americas Hylac® PL75 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D638 |
Polymer Resources PC/TP-GP3 PC/Polyester Alloy High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | 50 mm/min; ASTM D638 |
LG Chemical 20HRI GPPS Heat resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, S.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D638 |
Kostat ICP-STAT ICS-1004 PVC Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | 50 mm/min; ASTM D638 |
LG Chemical 20HRE GPPS High strength, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Sup.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D638 |
Kostat ICP-STAT ICD-1004 PVC Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D638 |
Techmer ES HiFill® PA6 0500 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM 638 |
PlastxWorld CEVIAN® B1700 PBT/ABS Alloy Unfilled, High Heat ResistantThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D638 |
Total PSC 524B Polystyrene Polystyrene 524B is a general purpose crystal polystyrene targeted for gloss coextrusion cap applications. It is specially formulated to reduce die buildup and die lines.Information provided by Tota.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D638 |
Total PSC 525 Polystyrene Polystyrene 525 is a crystal polystyrene for both injection molding and cap layer co-extrusion. Injection molding applications such as medical and laboratory parts, tumblers and jewel boxes demonstr.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3500 Natural 1050 Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 4011 HH Description: Ultra High Heat ABSInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 4500R Description: Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 4502 Description: Injection Molding Grade, Medium Impact Information provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 7500E Description: Extrusion Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 7602B Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D-638 |
Axiall 9109J Clear Rigid PVC, Extrusion, Clear Georgia Gulf 9109J Clear is designed for use in extruded price tag holders. The compound contains an ultraviolet light stabilizer, which retards color change.Information provided by Georgia GulfGeo.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D-638 |
Axiall HHP-190 Rigid PVC, Extrusion Georgia Gulf HHP-190 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Heat Resistance & Thermal StabilityImpact Strength & ToughnessDimensi.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D-638 |
Axiall HHW-191 Rigid PVC, Extrusion Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D-638 |
Axiall 8132 Rigid PVC, Extrusion Georgia Gulf 8132 is a rigid PVC compound designed for applications where transparency is important. This product remains unchanged except for the coded name and was previously identified as 3132. .. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D-638 |
Axiall 8258 Rigid PVC, Extrusion Georgia Gulf 8258 is a special purpose rigid PVC for film and food grade sheet compound. It has been used where packages are manufactured to FDA guidelines.Information provided by Georgia GulfGeorg.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D-638 |
Axiall Tuf-Stif 2804 Rigid PVC, Extrusion Georgia Gulf Tuf-Stif 2804 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit.. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM 638 |
PlastxWorld CEVIAN®-V 400N ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM Data |
Americas Styrenics Styron® 612 Polystyrene
(discontinued **) STYRON® 612 general purpose polystyrene resin is an easy flow resin with no color additives. When used unmodified for the manufacture of food contact articles STYRON 612 complies with the US Food, .. |