Kostat ICP-STAT ICD-1004 PVC Sheet

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Kostat
Trade Name ICP-STAT
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kostat ICP-STAT ICD-1004 PVC Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials based on Hygroscopic Antistats and Conductive Fillers. This product exhibits superior transparency and clarity.Special Features:Superior Permanent Static DissipationHumidity InsensitivityExcellent Wear resistanceLow Particle GenerationSuperior Transparency and ClarityLow Ionic ContaminationExcellent Chemical Resistance with Environmentally Friendly MaterialsApplications:Semiconductors PackagingLCD Components PackagingHDD Components PackagingElectrical & Electronics PackagingMedical Devices PackagingClean Room Accessories
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.2 MPa
6700 psi
ASTM D638
Optical Properties Metric English Comments
Transmission, Visible >= 90 %
>= 90 %
ASTM D1003
Electrical Properties Metric English Comments
Surface Resistivity per Square 1e+05 - 1.00e+6 ohm
1e+05 - 1.00e+6 ohm
ASTM D257
1.00e+6 ohm
1.00e+6 ohm
after 100% elongation; ASTM D257
1.00e+7 ohm
1.00e+7 ohm
after 200% elongation; ASTM D257
1.00e+9 ohm
1.00e+9 ohm
after 250% elongation; ASTM D257