Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PSC 525 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer Total Atofina
Trade Name PSC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PSC 525 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polystyrene 525 is a crystal polystyrene for both injection molding and cap layer co-extrusion. Injection molding applications such as medical and laboratory parts, tumblers and jewel boxes demonstrate the polymers ability to b e molded with minimal stresses and fast cycles. Utilizing 525 as a cap layer in cups, plates, and other consumer disposables takes advantage of this polymers melt rheology.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.2 MPa
6700 psi
ASTM D638
Tensile Modulus 3.03 GPa
440 ksi
ASTM D638
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 96.7 °C
206 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 101 °C
213 °F
ASTM D1525