Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall HHP-190 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall HHP-190 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Georgia Gulf HHP-190 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Heat Resistance & Thermal StabilityImpact Strength & ToughnessDimensional StabilityColorabilityUV Color StabilityFlame RetardantChemical ResistanceInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D-785
Hardness, Shore D 80
80
ASTM D-2240
Tensile Strength, Yield 46.2 MPa
6700 psi
ASTM D-638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D-638
Flexural Strength 76.5 MPa
11100 psi
ASTM D-790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D-790
Izod Impact, Notched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Gardner Impact 0.339 J
0.250 ft-lb
per mil; ASTM D-4226
Tensile Impact Strength 96.6 kJ/m²
46.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C
205 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
ASTM D-648
Flammability, UL94 V-1
V-1
At 0.065 inch
Processing Properties Metric English Comments
Zone 1 149 °C
300 °F
Zone 2 154 °C
310 °F
Zone 3 160 °C
320 °F
Zone 4 166 °C
330 °F
Zone 5 171 °C
340 °F
Die Temperature 177 °C
350 °F
Users viewing this material also viewed the following: