Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 44.1 MPa | 6400 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L1101 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L7416 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | ASTM D638 |
PTS Trilac® ABS-HS7500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ HTX M6215 Polyvinyl Chloride Alloy (PVC Alloy) It is recommended that the compound pellets be dried for 3 to 4 hours at 150 deg. F.Information provided by PolyOne |
|||
Tensile Strength, Yield | 44.1 - 75.0 MPa | 6400 - 10900 psi | Average value: 55.0 MPa Grade Count:12 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | ASTM D638 |
Ravago Manufacturing Americas Hylac® EX28 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 44.1 MPa @Thickness 3.20 mm |
6400 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 44.1 MPa @Thickness 3.20 mm |
6400 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical HF380U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 44.1 MPa @Thickness 3.20 mm |
6400 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Tensile Strength, Yield | 44.1 MPa @Thickness 3.20 mm |
6400 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Tensile Strength, Yield | 44.1 MPa @Thickness 3.20 mm |
6400 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | ASTM D638 |
Iran Petrochemical (PCC) SH-0150 Acrylonitrile Butadiene Styrene SH - 0150 ABS extrusion grade has been formulated to provide excellent mechanical properties,extrusion stability, vacuum formability and chemical resistance. It is a high flow extrusion grade with h.. |
|||
Tensile Strength, Yield | 44.1 MPa @Thickness 3.17 mm |
6400 psi @Thickness 0.125 in |
ASTM D638 |
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TX-0510 TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 44.1 MPa @Thickness 3.17 mm |
6400 psi @Thickness 0.125 in |
ASTM D638 |
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-0700FX ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-0926 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TX-0510 TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SIC 3710 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: High Impact ResistanceUses: Rigid Packing; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SRP 5902 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: High Gloss; High Impact Resistance Uses: Conduit; Piping; Profiles Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | ASTM 638 |
PlastxWorld CEVIAN®-V 660SF ABS High Flow ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 7401 Injection Molding Grade, Extra High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 44.1 MPa @Thickness 3.20 mm |
6400 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron IM-11B ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Tensile Strength, Yield | 44.1 MPa @Thickness 3.20 mm |
6400 psi @Thickness 0.126 in |
Type 1, 5 mm/min speed; ASTM D-638 |
Bhansali Engineering Abstron AP-78 EP ABS Electro Plating Applications Electroplating & Hot Stamping GradesInformation provided by Bhansali |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | ASTM D-638 |
Axiall 8264 Rigid PVC, Extrusion Georgia Gulf 8264 is a rigid PVC pellet compound suited for applications where transparency is important. 8264 is widely used for clear films, sheets, and profile shapes in the packaging industry. .. |
|||
Tensile Strength, Yield | 44.1 MPa @Thickness 3.20 mm |
6400 psi @Thickness 0.126 in |
Type 1; ASTM D638 |
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |
|||
Tensile Strength, Yield | 44.1 MPa @Thickness 3.20 mm |
6400 psi @Thickness 0.126 in |
Type 1, 5 mm/min speed; ASTM D-638 |
Bhansali Engineering Abstron SE-22 ABS Sheet Extrusion Grade Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali |
|||
Tensile Strength, Yield | 44.1 MPa @Thickness 3.20 mm |
6400 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron KU-650M ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Tensile Strength, Yield | 44.1 MPa | 6400 psi | ASTM D638 |
Polymer Resources PC/TP-GP3 PC Polyester, High Impact, Superior Chemical Resistance
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |