Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 42.7 MPa | 6190 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L4857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M5730 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M5731 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. Dark colored compounds do not.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | ASTM D638 |
Polymer Resources PC/TP-FR3 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | ASTM D638 |
Ravago Manufacturing Americas Hylac® HF96 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B930 (Base Grade), 4% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B932 (UV Inhibitor Added), 4% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9304 (Odor Mask Added), 4% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9324 (UVI, Odor Mask Added), 4% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | ASTM-D638 |
Ineos ABS Lustran® 427 |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | ASTM-D638 |
Ineos ABS Lustran® 451 ABS, Injection Molding Grade Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss. |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | ASTM D638 |
Spartech SP-9080 High Heat ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | ASTM D 638 |
Styrolution PS 3600/3601 GPPS Exceptional flow characteristicsGood for thin wall and complex partsUSP Class VI certifiedInformation provided by Styrolution |
|||
Tensile Strength, Yield | 42.7 MPa @Thickness 3.17 mm |
6200 psi @Thickness 0.125 in |
ASTM D638 |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 42.7 MPa @Thickness 3.17 mm |
6200 psi @Thickness 0.125 in |
ASTM D638 |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM Data |
Styron Magnum™ 9085 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM Data |
Styron Magnum™ 9450P ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 42.7 MPa @Thickness 3.17 mm |
6190 psi @Thickness 0.125 in |
|
TPI Porene® ABS-GA803 High Gloss, UV Resistant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3501 Black 1302 Injection Molding Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 9301 Description: Extrusion Grade, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | ASTM D638 |
Engineered Polymer Solutions ABS 550 Medium Impact. Natural and colors available. Medium gloss. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions. |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 7501 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | ASTM D-638 |
Axiall 2502 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | ASTM D-638 |
Axiall 2506 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | ASTM D-638 |
Axiall 7048A Rigid PVC, Extrusion Georgia Gulf 7048A is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityCert.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | ASTM D-638 |
Axiall 9153 Rigid PVC, Molding Georgia Gulf 9153 is an excellent combination of chemical resistance, impact and processing for chemically active products, such as pine oil cleaners.Information provided by Georgia GulfGeorgia Gulf.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6200 psi | ASTM D-638 |
Axiall 2503 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM Data |
Styron Magnum™ 3490 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |