Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 40.0 MPa | 5800 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® GPM5500S ABS (Europe-Africa-Middle East) CYCOLAC GPM5500S is a multi purpose injection moulding grade, equal to GPM5500 but equiped with anti static agents, providing a favourable balance of engineering properties. CYCOLAC GPM5500S has a w.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® HMG94MD ABS Superior flow, injection molding ABS for medical applications. Good impact. For thin-wall applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East) CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR8510 ASA ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
Tensile Strength, Yield | 40.0 - 65.0 MPa | 5800 - 9430 psi | Compression; ISO 527 |
Raschig Group MELOPLAS® 183 MF Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Faradex AS0029 ABS (Europe-Africa-Middle East) LNP* Faradex* AS-1002 FR is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: Flame Retardant, EM.. |
|||
Tensile Strength, Yield | 40.0 MPa @Temperature 23.0 °C |
5800 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT
(Unverified Data**) Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | 50 mm/min |
Polimeri Europa KOBLEND HI 18 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend, similar to KOBLEND HI 10 with improved impact resistance at low temperatures and better thermal properties. Main applicat.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | ASTM D638 |
Ineos Nova 3601 General Purpose Crystal Polystyrene
(discontinued **) Easy flow for high productivity, excellent post molding scuff resistanceApplications: Medical, LabwareExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phys.. |
|||
Tensile Strength, Yield | 40.0 - 82.0 MPa | 5800 - 11900 psi | Average value: 53.2 MPa Grade Count:11 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | ASTM D638 |
Ineos ABS Lustran® 228 Specialty, High Productivity
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | ASTM D638 |
BP Amoco Amoco® 7556 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: High speed spinning, Improved bulk, Low gas fadeTypical applications: Upholstery, BCF carpet yarnsComplies with FDA specification, Title 21, CF.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | ASTM D638 |
Ravago Manufacturing Americas Hysun™ 693 ASA
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | 2 in/min; ASTM D638 |
BASF Capron® 8224 HSL Nylon 6 (Conditioned)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | ISO R527 |
Fainplast Compounds RH 214 Rigid PVC, Antishock Extrusion Antishock rolling shutters |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | ISO R527 |
Fainplast Compounds RH 225 Rigid PVC, Antishock Extrusion Antishock pipes and profiles |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | ISO R527 |
Fainplast Compounds RKS 320 Rigid PVC, Antishock Extrusion Lead Free Various profiles, antishock |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | ASTM D638 |
IRPC Polimaxx Polene 1111R Polypropylene Homopolymer CHARACTERISTICS: EXCELLENT HIGH STIFFNESS, HEAT STABILITY, HIGH FLOW CONTAIN LONG TERM HEAT AGING ADDITIVE APPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES, COFFEE MAKER, HAIR DRYER |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | ISO-DIS 527 |
Schwartz Technical Plastics LAMIGAMID® 410 Cast Polyamide 6, Elastomer Modified, Low Temp, Dry Application: outrigger floats, rollersInformation provided by Schwartz Technical Plastics GmbH |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | 50mm/min; ISO 527 |
Styrolution Terblend® N NMX04 ABS/PA6 (Dry) Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12 4.3 specific gravity nylon 12, clean compound system |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 nat PA12 Medium viscosity unmodified Polyamide 12Information provided by EMS Grivory |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | 50 mm/min, 4 mm; ISO 527 |
Chi Mei Kibiton® PB-5900 Styrene-Butadiene Copolymer Injection Molding, High rigidity |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | ASTM D638 |
Braskem H 105 Injection Molding Polypropylene Description: H 105 is a high melt flow rate homopolymer with high transparency. Designed for use on thin-walled injection molding parts with high output. This product exhibits excellent processabili.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | ISO 527-1 |
Barlog Plastics KEBAFORM C 906 UR POM Copolymer unreinforced, impact modified POM-IInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | |
Addcomp PRIEX® 20070 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 40.0 MPa | 5800 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR7500 ASA (Asia Pacific) High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |