Addcomp PRIEX® 20070 Maleic Anhydride Grafted PP homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Addcomp
Trade Name PRIEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addcomp PRIEX® 20070 Maleic Anhydride Grafted PP homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural fibers and polyolefin in reinforced polyolefin blendsImprove homogeneity of mineral, clay or pigment dispersion in compoundsBroaden the temperature range of composite applicationsInformation provided by Addcomp Polymer Additive Solutions
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
Elongation at Break 11 %
11 %
Tensile Modulus 2.05 GPa
297 ksi
Thermal Properties Metric English Comments
Melting Point 160 - 164 °C
320 - 327 °F
Crystallization Temperature 113 - 115 °C
235 - 239 °F
Deflection Temperature at 0.46 MPa (66 psi) 121 - 129 °C
250 - 264 °F
Descriptive Properties Value Comments
Oxygen induction time 35-50 min
Users viewing this material also viewed the following: