Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50 mm/min; ISO 527 |
Polimeri Europa Edistir RK 5512G Polystyrene UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal properties. It exhibits a good stability to the processing conditions and to the light
exposure.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50mm/min; ASTM D638 |
Reliance Industries Repol C080MT Polypropylene REPOL Polypropylene C080MT is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO R527 |
Solvay Engineered Polymers SEQUEL® 2330 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2330 engineered polyolefin is designed for large mold-in-color automotive interior applications that require stiffness and good dimensional stability. This material exhibits e.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50 mm/min |
Polimeri Europa EDISTIR PD RK5512G High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-23 UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal pr.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3330 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 25 PHR Tricresyl Phosphate MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
Chevron Phillips HiD® 9348 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 335440A; ASTM D 4976 Classification: PE 235, A 56606Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
Global GA-3245 High Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- shopping bags, packing bagsInformation provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50 mm/min |
Eastman Tenite 264-16 CAB Cellulose Acetate Butyrate
(discontinued **) 16% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
Flint Hills AP6120-HS Impact Copolymer Polypropylene High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: appliance components, automotive interior trim, and consumer durables.Former Huntsma.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 2 in/min.; ASTM D638 |
Ineos A4040 HDPE Ineos HDPE A4040 is a high density polyethylene copolymer produced using a supported catalyst process. It is a copolymer resin used mainly for the extrusion of crosslinked pipes according to the sil.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638-02 |
Ipiranga Petrochem HD 7555 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
LyondellBasell Astryn 73F5-1 Polypropylene Copolymer, 10% Calcium Carbonate Key Features: medium high melt flow, medium modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good colorability, good aesthetics, very good processabilityAppli.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638-02 |
Ipiranga Petrochem GM 7040 G HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527-1, -2 |
LyondellBasell Hifaxâ„¢ DR279 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ DR279 high melt flow, 1,200 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has a unique balance of stiffness, impact resistance, processability.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | |
Silon Tabond 3012 Adhesive Resin TABOND 3012 is an LLDPE based adhesive resin.Characteristics: • Highest adhesion to aluminium, copper, brass and steel • Adhesion durability at elevated temperatures and pressure cycling p.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific) LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50mm/min; ISO 527-2 |
Borealis Daplen™ EE158AI Polypropylene TPO Compound Daplen™ EE158AI is a 13% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50mm/min; ISO 527-2 |
Borealis PS65C40 Polypropylene Compound, Mineral Filled PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
Videolar 825 E High Impact Polystyrene (HIPS) Grade designed specially for extrusion and thermoformingCharacteristics make it especially suitable for industrial packaging deep draw thermoforming and custom multilayer sheet extrusionFeatures: St.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50 mm/min; ISO 527 |
Chi Mei Polyrex® PH-55Y Polystyrene - Food Medium impact |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP25-1202 TF20 20% Talc Filled Copolymer Polypropylene, Impact Modified, High Heat, High Stiffness with UV and Paintable Versions Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527 |
Eurostar Starflam M10009XP PP, Flame Retardant, Injection Molding Starflam M10009XP is an Unfilled Flame Retardant Polypropylene (Copolymer) Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM-D638 |
Braskem GM7746CA HDPE Blow Molding Polyethylene GM7746CA is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tena.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | Typical; ISO 527-1/2 |
Axion Polymers Axpoly® PS02 1010 Medium Impact Polystyrene PS02 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin co.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | |
BASF Procom® D 1158 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | |
BASF Novolen® 3300 MC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50 mm/min |
Arkema Group Orgalloy® LT 5050T Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good .. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
Carmel Olefins CARMELTECH™ QB 79 P Polypropylene Random Copolymer for Pressure Pipe CARMELTECH™ QB 79 P is a high molecular weight, low melt flow rate polypropylene random copolymer, especially designed for extrusion of pressure pipes and injection molding of fittings. This grade .. |