Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527 |
Idemitsu Kosan Xarec® EA 528 SPS, 30% Glass Filled
(discontinued **) Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 420SE0 PBT 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 420SE0 PBT 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 420SE0U PBT PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized |
|||
Tensile Strength, Yield | 120 MPa @Strain 0.200 %, Temperature 300 °C |
17400 psi @Strain 0.200 %, Temperature 572 °F |
Annealed prior to test |
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570Â.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM D638 |
SPS Guang Zhou POLLITEâ„¢ 1002G30 Flame-retarded/GF30%-Polycarbonate Characteristic: High mechanical properties, high rigidity, high heat resistant, good dimensional stability, good flame retardanceApplications: E/E parts, power tool, office suppliesInformation Provi.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP LF002 PEEK LNP* THERMOCOMP* LF002 is a compound based on Polyetheretherketone resin containing 10% Glass Fiber. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp WF007 PET/PBT LNP Thermocomp WF-1007 BK8-114 is a compound based on PET/PBT resin containing glass fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM D638 |
Techmer ES Electrablend® PA6 GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by Weight/Unspecified Filler/Reinfor.Additive: LubricantFeatures: Conductive and LubricatedAppear.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific) Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM-D638 |
Polyram PlusTek PB302G3 Nylon 6, 15% Glass Fiber 15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM-D638 |
Polyram RamSter PF320G4 PBT, 20% Glass Fiber, Flame Retardant 20% Glass fiber reinforced, flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | GB/1040 |
Zhejiang Juner PA-A6-66H High CTI Value Halogen-Free Environmental Protection Flame-Resistant and Reinforced Polyamide Applications: Cover of Mini MCBInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527 |
Polyram PlusTek PD304G6YL55 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced 30% Glass-fiber reinforced Nylon 12 for injection molding applications. UL listed.Information provided by Polyram. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527 |
Polyram Polytron P40N11 Polypropylene, 40% Long Glass Fibers A chemically coupled 40% long glass fiber reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM D638 |
Aclo Accutech Nylon 6 NY0730G20L Glass Reinforced |
|||
Tensile Strength, Yield | 120 MPa @Temperature -40.0 °C |
17400 psi @Temperature -40.0 °F |
ISO 527 |
BASF Ultramid® 8200 HS PA 6 (Conditioned) Description: Ultramid 8200 HS is a heat stabilized, medium viscosity, PA6 injection molding homopolymer, exhibiting resistance to sink-mark formation in thick sections, and improved toughness over c.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Tensile Strength, Yield | 120 MPa @Strain 0.200 %, Temperature 871 °C |
17400 psi @Strain 0.200 %, Temperature 1600 °F |
|
AK Steel 309 Austenitic Stainless steel AK Steel 309 provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic wh.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl.. |
|||
Tensile Strength, Yield | 120 MPa @Strain 0.200 %, Temperature 982 °C |
17400 psi @Strain 0.200 %, Temperature 1800 °F |
|
Haynes 230® alloy, cold rolled and 1232°C solution annealed sheet Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |