| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | MD; ASTM D955 |
| Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 113 | 113 | ASTM D785 |
| Tensile Strength at Break | 117.0 MPa | 16970 psi | ASTM D638 |
| Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM D638 |
| Elongation at Break | 8.0 % | 8.0 % | ASTM D638 |
| Elongation at Yield | 5.0 % | 5.0 % | ASTM D638 |
| Tensile Modulus | 3.699 GPa | 536.5 ksi | ASTM D638 |
| Flexural Strength | 187.0 MPa | 27120 psi | ASTM D790 |
| Flexural Modulus | 5.999 GPa | 870.1 ksi | ASTM D790 |
| Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F |