Polymer Property : Tensile Strength, Yield = 116 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 116 MPa
16800 psi
ISO 527-2
PolyOne Nymax™ GMF 604 40 UV Black 28 Polyamide 6 (Nylon 6)
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor..
Tensile Strength, Yield 116 MPa
16800 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC
LNP* LUBRICOMP* DFL369XF is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant.
Tensile Strength, Yield 116 MPa

@Temperature 22.8 °C
16800 psi

@Temperature 73.0 °F
ASTM D638
Ensinger Sintimid™ V-HPHT high purity high temp Polyimide (PI)  (discontinued **)
SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V..
Tensile Strength, Yield 116 MPa
16800 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK
LNP* Lubricomp* LFL36 is a compound based on PEEK containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength, Yield 116 MPa
16800 psi
SABIC - Japan Method
SABIC Innovative Plastics Valox® PDR4911 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Strength, Yield 116 MPa
16800 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® V4860HR PBT
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
Tensile Strength, Yield 116 MPa
16800 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF/M40 HS L NAT 40% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures..
Tensile Strength, Yield 116 MPa
16800 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF/M40 HS Up BK 40% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat Sta..
Tensile Strength, Yield 116 MPa
16800 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF/M40 IG BK 40% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures..
Tensile Strength, Yield 116 MPa
16800 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF/M40 L BK 40% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures..
Tensile Strength, Yield 116 MPa
16800 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC
LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features include: Electrically Conductive, Easy Molding, Mold Release.
Tensile Strength, Yield 116 MPa
16800 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC
LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features include: Electrically Conductive, Easy Molding, Mold Release.
Tensile Strength, Yield 116 MPa
16800 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC (Asia Pacific)
LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Mold Release.
Tensile Strength, Yield 116 MPa
16800 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC (Asia Pacific)
LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Mold Release.
Tensile Strength, Yield 116 MPa
16800 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DF006RXQ PC
LNP* THERMOCOMP* DF006RXQ is a compound based on Polycarbonate resin containing 30% Glass Fiber.
Tensile Strength, Yield 116 MPa
16800 psi
SABIC - Japan Method
SABIC Innovative Plastics NORYL HM4025H PPE+PS (Asia Pacific)
40% GF/MF filled FR PPE/PS blend, high flow
Tensile Strength, Yield 116 MPa
16800 psi
Type I, 10 mm/min; SABIC - Japan Method
SABIC Innovative Plastics NORYL PCN2615 PPE+PS (Asia Pacific)
Tensile Strength, Yield 116 MPa
16800 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® V4860HR PBT (Asia Pacific)
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
Tensile Strength, Yield 116 MPa
16800 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East)
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
Tensile Strength, Yield 116 MPa
16800 psi
ISO 527
Polyram PlusTek PA840G13 Nylon 66 for Injection Molding, 13% Glass Fiber Reinforced, Impact Modified, Heat Resistant
Impact modified, 13% glass fiber reinforced, heat resistant Nylon 66 for injection molding applications.Information provided by Polyram.
Tensile Strength, Yield 116 MPa

@Temperature 23.0 °C
16800 psi

@Temperature 73.4 °F
EN ISO 527
Ensinger TECASINT 1011 Polyimide (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Tensile Strength, Yield 116 MPa

@Temperature -40.0 °C
16800 psi

@Temperature -40.0 °F
ASTM Test
BASF Ultramid® 8253 HS PA6 (Conditioned)
Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased..
Tensile Strength, Yield 116 MPa

@Temperature -40.0 °C
16800 psi

@Temperature -40.0 °F
ISO Data
BASF Ultramid® 8253 HS PA6 (Conditioned)
Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased..
Tensile Strength, Yield 116 MPa

@Temperature -40.0 °C
16800 psi

@Temperature -40.0 °F
ASTM Test
BASF Ultramid® 8253 PA6 (Conditioned)
Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o..
Tensile Strength, Yield 116 MPa

@Temperature -40.0 °C
16800 psi

@Temperature -40.0 °F
ISO Data
BASF Ultramid® 8253 PA6 (Conditioned)
Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o..
Tensile Strength, Yield 116 MPa
16800 psi
ASTM D638
Ashley Polymers Ashlene® P126 PBT Polyester, 30% Glass Reinforced
PBT polyester with 30% glass reinforcement.Data provided by the manufacturer
Tensile Strength, Yield 116 MPa
16800 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC
LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated, Easy Molding.
Tensile Strength, Yield 116 MPa
16800 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC (Asia Pacific)
LNP* Lubricomp* DFL369XF is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant.