Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 23 I Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 I represents the version of Flexirene FG 20 I.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 23 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 U represents the version of Flexirene FG 20 U.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-D LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CM 406 are characterized by h.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-Y821-D Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Good stiffness and machinability, good blocking resistance.Applications: Bags-on-roll, produce bags, garment film, trash bags.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527 |
Total Finathene® LL 4010 FH 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527 |
Total Finathene® LL 6010 FH 18P LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527 |
Total Finathene® LL 6010 FE 18P LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil Escorene® LD-138 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin offering good clarity, toughness, and stiffness. Blown film made from this resin has good machinability in bag equipment a.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-0118-F Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Stretch wrap, blend resin, industrial packaging.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
LyondellBasell Montell 16501F3 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
LyondellBasell Montell 16501F8 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
LyondellBasell Montell 16502F8 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527 |
Iran Petrochemical (PCC) LS0085 Low Density Polyethylene LS0085 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: thin shrink film.Information provided.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527-3 |
Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film LL 1810 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 H can be processed at high o.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LD 071.LR Blown Film Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LD 124.MS General Purpose Clarity Film Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 051.LQ Low Density Polyethylene Resin Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding proc.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 100.BW Low Density Polyethylene Resin Product Description: LD 100.BW is a LDPE grade, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.Ava.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | |
Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045.11 Polyethylene resin is a premier film resin for general purpose packaging applications, ranging from heavy duty applications to high speed, thin gauge applications. It contains high .. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | |
Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade DOWLEX® 2077 Polyethylene resin is a fully formulated linear low density polyethylene resin designed for use in food packaging applications. This blown film resin is designed to run on narrow die-g.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | |
Dow LDPE 170A Low Density Polyethylene, Blown Film Grade DOW LDPE 170A resin is used for shrink and heavy duty blown film applications where optical clarity is desired. It contains medium level of antiblock additives. It complies with U.S. FDA regulation .. |