Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex CL 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 106 are characterized by h.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 208 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LFH.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
SABIC 118 Series Linear Low Density Polyethylene for Blown Film Product Description: 118 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. Films produced using these resins yield good tensile properties, impact st.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
SABIC 120W Linear Low Density Polyethylene for Blown Film Product Description: 120W is a Linear Low Density Polyethylene grade suitable for general purpose packaging. Films produced using this resin yield good tensile properties, impact strength and opti.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 20 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 U is recommended for the .. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Riblene® FC 30 Low Density Polyethylene - Blown Film Extrusion Riblene FC 30 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 30 is characterized by a high melt strength leading to a good bubble sta.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 29 Low Density Polyethylene - Blown Film Extrusion Riblene FF 29 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 29 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
Polimeri Europa Riblene® FH 10 Low Density Polyethylene - Blown Film Extrusion Riblene FH 10 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 10 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin Film Properties. Features: Free flowing granules, toughness and strength, ease of extrusion.Applications: Blending, concentrates.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0219-A LDPE Foam Resin Features: Good heat sealing latitudeModerate toughnessEasy processability Applications: Industrial packagingLinersBlends with LLDPEFoam ArticlesInformation provided by Nova Chemicals |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0219-A LDPE Film Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinInformation provided by NOVA Chemi.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0323-B LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Bakery bags, sandwich bags, zipper lock bags, cast film.Data provide.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® TD-9022-D Super Hexene Film Resin Excellent dart impact, High strength, High toughnessApplications: Retail trash bagsAdditives: Process stabilizer, Slip/antiblockFilm properties are typical of blown film extruded at a blowup ratio o.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Sclair® FP120-D Octene LLDPE Film Resin Applications: Food packaging, freezer film, lamination and sealant filmInformation provided by Nova Chemicals |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D 882 |
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 75 Micron Film FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Sclair® 11Q4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0218-B Butene Copolymer LLDPE Film Resin PF-0218-B complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0218-E Butene Copolymer LLDPE Film Resin PF-0218-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-0218-F Butene LLDPE Film Resin Toughness and strength, Ease of extrusionApplications: Cast films, BlendingAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depende.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-0218-J Butene LLDPE Film Resin Film Properties. Features: High MI for easier extrusion.Applications: Trash bags, general purpose packaging, garment film.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y822-CP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness, suitable for narrow die gaps.Applications: Heavy duty sacks, high strength packaging.Data provided by the manufac.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0209 AA LLDPE Film Applications:Heavy duty sacksAgricultural films and linersProduce bags, stretch filmFilm properties were measured on 15 micron film extruded at a blow up ratio of 2:1.Information provided by Interch.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0220 AA LLDPE Film Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 1184 |
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l... |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | 2 in per min; ASTM D882 |
Chevron Phillips MarFlex® D139 m-LLDPE Linear Low Density Polyethylene Low Density PolyethyleneCustomer Benefits: Possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved processability (bubble stability, down-.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
Dow FLEXOMER™ ETS-9066 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
ExxonMobil Escorene® LD-332 EVA Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1% vinyl acetate copolymer packaging film resin. Film made from LD-332 offers improved impact strength and heat sealability compared to homopolym.. |
|||
Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0218-AF LDPE Extrusion Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |