| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
| Polimeri Europa Clearflex® H&T CLH 150 Linear Low Density Polyethylene Clearflex H&T CLH 150 is a linear low density polyethylene resin, with antioxidants, suitable for cast film extrusion.Stretch films obtained from Clearflex H&T CLH 150 show good optical properties, .. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
| Polimeri Europa Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 208 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LFH.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| SABIC 120W Linear Low Density Polyethylene for Blown Film Product Description: 120W is a Linear Low Density Polyethylene grade suitable for general purpose packaging. Films produced using this resin yield good tensile properties, impact strength and opti.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
| Polimeri Europa Flexirene® FG 20 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 U is recommended for the .. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
| Polimeri Europa Riblene® FC 20 Low Density Polyethylene - Blown Film Extrusion Riblene FC 20 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 20 is characterized by a high melt strength leading to a good bubble sta.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
| Polimeri Europa Riblene® FC 30 Low Density Polyethylene - Blown Film Extrusion Riblene FC 30 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 30 is characterized by a high melt strength leading to a good bubble sta.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
| Polimeri Europa Riblene® FF 22 Low Density Polyethylene - Blown Film Extrusion Riblene FF 22 is a high molecular weight low density polyethylene (LDPE), with added slip agent, suitable for blown film extrusion. Riblene FF 22 is characterized by a good melt strength leading to.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
| Polimeri Europa Riblene® FF 29 Low Density Polyethylene - Blown Film Extrusion Riblene FF 29 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 29 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
| Polimeri Europa Riblene® FF 30 Low Density Polyethylene - Blown Film Extrusion Riblene FF 30 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 30 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
| Polimeri Europa Riblene® FL 20 Low Density Polyethylene - Blown Film Extrusion Riblene FL 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FL 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 527-3 |
| Polimeri Europa Riblene® FM 23 Low Density Polyethylene - Blown Film Extrusion Riblene FM 23 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 23 is characterized by a good balance between processabilit.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| NOVA Chemicals Novapol® LA-0219-A LDPE Foam Resin Features: Good heat sealing latitudeModerate toughnessEasy processability Applications: Industrial packagingLinersBlends with LLDPEFoam ArticlesInformation provided by Nova Chemicals |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| NOVA Chemicals Novapol® PF-Y821-CP Butene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE Puncture value is 60 J/mm. Additive Package: Antiblock.Applications: industrial liners, heavy duty packaging.Film properties are typical of 25 µm blown film extruded at a blow-up ratio of 2.5:1, b.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D 882 |
| NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 75 Micron Film FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| SABIC HP0722N Low Density Polyethylene for Blown Film Product Description: HP0722N is a Low Density Polyethylene grade suitable for producing medium duty films and contains no slip or antiblock additives. It yields good toughness and optical properti.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Strength and toughness, good sealing properties, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| NOVA Chemicals Sclair® 12J1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity.Applications: Overwrap, lamination.Data provided by the manufacturer. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 1184 |
| Iran Petrochemical (PCC) Tabriz 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| NOVA Chemicals Novapol® PF-0218-F Butene LLDPE Film Resin Toughness and strength, Ease of extrusionApplications: Cast films, BlendingAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depende.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882-02 |
| Ipiranga Petrochem LB 0316 LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 1184 |
| SIDPEC EGYPTENE® LL 0209 AA LLDPE Film Applications:Heavy duty sacksAgricultural films and linersProduce bags, stretch filmFilm properties were measured on 15 micron film extruded at a blow up ratio of 2:1.Information provided by Interch.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 1184 |
| SIDPEC EGYPTENE® LL 0220 AA LLDPE Film Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ISO 1184 |
| SIDPEC EGYPTENE® LL 0220 KJ LLDPE Film Applications: Light and medium duty film.Film properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor of Sidi Ke.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| Dow FLEXOMER™ ETS-9066 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| NOVA Chemicals Novapol® TF-0119-FP Hexene LLDPE Film Resin
(discontinued **) Film Properties. Features: High strength and toughness, low gel count, intended for narrow die gaps.Applications: Stretch wrap, blend resin.Data provided by the manufacturer. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| NOVA Chemicals Sclair® 11N1 PE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depe.. |
|||
| Film Tensile Strength at Yield, MD | 10.0 MPa | 1450 psi | ASTM D882 |
| NOVA Chemicals Novapol® LF-0218-AF LDPE Extrusion Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |
|||