Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 14.3 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CY5105 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP ..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS
PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific)
PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East)
PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Europe-Africa-Middle East)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer
Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Asia Pacific)
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer
Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Europe-Africa-Middle East)
Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)
Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.I..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 80
LG Chemical PI-642 ABS, Fitting, High Strength
Information Provided by LG Chem
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -20.0 °C
14.3 ft-lb/in²

@Temperature -4.00 °F
ISO 180/4A
Mitsubishi Xantar® C CM 206 Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
cond.; ISO 180-1A
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified
PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS.
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -20.0 °C
14.3 ft-lb/in²

@Temperature -4.00 °F
ISO 180/4A
Mitsubishi Xantar® C CM 206 U Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -20.0 °C
14.3 ft-lb/in²

@Temperature -4.00 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® CL500U PBT+PC (Europe-Africa-Middle East)
XENOY CL500U is a semi-crystalline blend, developed for exterior automotive parts ( except bumper shells ) and non automotive parts, requiring good impact, excellent chemical resistance and UV stabi..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -10.0 °C
14.3 ft-lb/in²

@Temperature 14.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® XD549S PBT+PC (Europe-Africa-Middle East)
Xenoy XD549S is an automotive grade, designed for thin wall (2.5 mm.) direct gated exterior parts. The material has an excellent flow. Xenoy XD549S can be painted with primerless solvent or waterbas..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Sax Polymers SAXLAC 310T Acrylonitrile Butadiene Styrene
Saxalac 310T is an antistatic, high impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Sax Polymers SAXLAC 310U Acrylonitrile Butadiene Styrene
Saxalac 310U is an antistatic, high impact resistant and light stabilized ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% ..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1A
Eurostar Star X 1615 33V S4 PA66, Glass Fiber Reinforced, UV stabilized, Injection Molding
Star X 1615 33V S4 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -40.0 °C
14.3 ft-lb/in²

@Temperature -40.0 °F
Edgew 80x10x4 sp=62; ISO 180/1A
Eurostar Staramide AST43 PA66, Impact Modified, Injection Molded
AST43 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Eurotec® Tecotek® BC40 UF65 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, standard grade
Information provided by Eurotec®
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 66Z Nylon 66, Conditioned
Vydyne® 66Z is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66Z resin offers high strength, rigidity and toug..
Izod Impact, Notched (ISO) 30.0 kJ/m²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 67R Nylon 66, Heat Stabilized, Conditioned
Vydyne® 67R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67R resin offers high strength, ..
Copyright © lookpolymers.com All Rights Reserved