| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | Eurotec |
| Trade Name | Tecotek® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Eurotec® Tecotek® BC40 UF65 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, standard grade.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527 |
| Elongation at Break | >= 50 % | >= 50 % | ISO 527 |
| Tensile Modulus | 2.25 GPa | 326 ksi | ISO 527 |
| Izod Impact, Notched (ISO) | 30.0 kJ/m² <br>@Temperature -30.0 °C |
14.3 ft-lb/in² <br>@Temperature -22.0 °F |
ISO 180/1A |
| 50.0 kJ/m² <br>@Temperature 23.0 °C |
23.8 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB <br>@Temperature 23.0 °C |
NB <br>@Temperature 73.4 °F |
ISO 180/1U |
| NB <br>@Temperature -30.0 °C |
NB <br>@Temperature -22.0 °F |
ISO 180/1U |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 110 °C | 230 °F | ISO 75 |
| Vicat Softening Point | 120 °C <br>@Load 5.10 kg |
248 °F <br>@Load 11.2 lb |
ISO 306 |
| Flammability, UL94 | HB <br>@Thickness 0.750 mm |
HB <br>@Thickness 0.0295 in |
|
| HB <br>@Thickness 1.60 mm |
HB <br>@Thickness 0.0630 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+15 ohm | 1.00e+15 ohm | IEC 60093 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 240 - 260 °C | 464 - 500 °F | |
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
| Drying Temperature | 80.0 - 100 °C | 176 - 212 °F | |
| Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
| Hold Pressure | 50.0 - 100 MPa | 7250 - 14500 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Back Pressure | Low | |
| Injection Speed | Medium - Fast |