Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXG154 PC FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East) XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS 240 Injection Molding Grade Lustran® ABS 240 has standard impact strength and is injection molding grade. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Europe-Africa-Middle East) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® EXXY0112 PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXAMID 226F8 Nylon 6.6, 40% Glass Fiber SAXAMID 226F8 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 40% glass fibers. It has very high mechanical strength.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl PKN4736 PPE+HIPS (Europe-Africa-Middle East) NORYL PKN4736 is a PPO+HIPS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food contact regulations.This .. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Asia Pacific) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Sax Polymers SAXATEC 4307 Acrylonitrile Styrene Acrylate SAXATEC 4307 is a high impact resistant, high viscosity and weatherable ASA injection molding grade, characterized by high mechanical strength and good processabilityInformation provided by SAX Poly.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
7.61 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Thickness 3.20 mm, Temperature -30.0 °C |
7.61 ft-lb/in² @Thickness 0.126 in, Temperature -22.0 °F |
complete break; b.o. ISO 180-A |
Covestro Makrolon® 3258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -40.0 °C |
7.61 ft-lb/in² @Temperature -40.0 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -40.0 °C |
7.61 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG6ST43H PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding Staramide AG6ST43H is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecoform® PO20 NL IL POM, impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 GR30 NL PA 6 30% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 GR30 NL HW PA6, 30% glass fiber reinforced, hydrolysis stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47 Nylon 66, DAM Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 KK30 NL IL PA 6 30% glass fiber/mineral reinforced, impact modified, low warpage Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 73G30TGI BK267 Nylon 6
(Unverified Data**) Zytel® 73G30TGI BK267 is a 30% glass fiber reinforced, toughened, black polyamide 6 optimized for gas injection molding process.Information provided by DuPont Performance Polymers |