Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 121R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. Internal mold release. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HF1110R PC (Europe-Africa-Middle East) LEXAN HF1110R is a high flow grade especially designed for applications that require thin wall sections and high flow lengths. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Asia Pacific) 19 MFR LEXAN High Flow Ductile Copolymerwith 400 nm cut off, available in transparent colors only |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPXS8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Europe-Africa-Middle East) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 143X PC Copolymer (Asia Pacific) Improved flow PC with excellent processability and mold release. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML3729 PC (Europe-Africa-Middle East) LEXAN ML3729 is an UV stabilized grade, with an excellent flow. It contains a release agent to ensure easy processing. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Lanxess Durethan® BKV 140 DUS008 000000 Nylon 6, 40% Glass Fiber PA 6, 40% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRILOY UX99725 PPA LNP LUBRILOY* UX99725 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON SE002Z PA 12 (Asia Pacific) LNP* Stat-kon* SE002Z is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 LNP* STAT-KON* SE003 is a compound based on Nylon 12 resin containing 15% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Asia Pacific) LNP* Thermocomp* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 (Europe-Africa-Middle East) Heat stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GFN2 PPE+PS PPE+PS blend. 20% Glass reinforced. UL746C F1. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional sta.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL N110HG PPE+HIPS (Europe-Africa-Middle East) NORYL N110HG is an unfilled material, with a Vicat B/120 of 116°C according ISO 306. NORYL N110HG can be used in applications where high gloss is required. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP QC008 PA6.10 LNP* THERMOCOMP* QC008 is a compound based on Nylon 6/10 containing 40% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP RC006H PA 66 LNP THERMOCOMP* RC006H is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP SH1100A PA12 LNP* Thermocomp* SH1100A is a Nylon 12, High Specificy Gravity compound containing proprietary fillers. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® NB1803E-BK Nylon/Polypropylene Alloy Description: Nylon/Polypropylene AlloyInformation provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | ISO 180 |
Polyram RamShine PS580 High Impact Polystyrene, Flame Retardant Flame retardant V-0, high impact polystyrene for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Star L PA6 30V D61 PA6, Glass Filled, Injection Molding Star L PA6 30V D61 is a PTFE/Silicone Oil Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-777E ABS - High Heat Ultra High Heat |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl C2 V15 Nylon 66/6, 15% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp FF004 PE (Europe-Africa-Middle East) LNP* THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |