Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP FARADEX MS002 PP LNP* FARADEX* MS002 is a compound based on Polypropylene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp HX05073 PA 11 LNP THERMOCOMP* HX05073 is a compound based on Nylon 11 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP YF006A Polyester Elastomer (Europe-Africa-Middle East) LNP* THERMOCOMP* YF006A is a compound based on Polyester Elastomer containing Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON MV008 PP (Europe-Africa-Middle East) LNP* VERTON* MV008 is a compound based on Polypropylene resin containing Long Glass. Added features include Chemically Coupled. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON MV008S PP (Asia Pacific) LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON MV008SU PP LNP VERTON* MV008SU is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -20.0 °C |
11.9 ft-lb/in² @Temperature -4.00 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -20.0 °C |
11.9 ft-lb/in² @Temperature -4.00 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Europe-Africa-Middle East) PPX7110 is an alloy of PP and PPO, providing high impact and good heat resistance. Generic identification acc. ISO11469: >PP+PPE+PS-I |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX1180 PPE+HIPS (Europe-Africa-Middle East) Noryl* PX1180 PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is an unfilled , injection moldable grade, with improved impact performances, an ISO 306 Vicat B/120 temperature of 120 deg C and a.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX1181 PPE+HIPS (Europe-Africa-Middle East) Noryl* PX1181 PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is an unfilled , injection moldable grade, with improved impact performances, an ISO 306 Vicat B/120 temperature of 120 deg C and a .. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton OX07411 PPS (Asia Pacific) LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO 180 |
Polyram PlusTek PA804 Nylon 6.6 for Injection Molding, Impact Modified Impact modified Nylon 6.6 for injection molding application.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO 180 |
Polyram Polytron P50B07 Polypropylene, 50% Long Glass Fiber, UV Stabilized A chemically coupled 50% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO 179 |
Total PPC 4640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4640 is a nucleated copolymer. PPC 4640 is characterized by good stiffness and impact resistance coupled with high creep resistance. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | Low Temp; ISO 180/1eA |
Lubrizol ESTALOC® 59200 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecolen® CP20 GR20 NL XC30 PPCP, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO Test |
BASF Ultramid® B3ZG7 OSI BK23273 35% Glass Filled PA6 (Dry) Ultramid B3ZG7 OSI BK23273 is a 35% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet demanding mechanical and chemical requi.. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl PMD 20164 Nylon 6 High resistance to repeated impactsInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON MV008SXP PP (Europe-Africa-Middle East) LNP* Verton* MV008SXP is a compound based on Polypropylene resin containing Long Glass. Added features include: Chemically Coupled, Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 25.0 kJ/m² @Temperature -40.0 °C |
11.9 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV007ES PA 66 LNP VERTON* RV007ES is a compound based on Nylon 66 resin containing 35% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |