Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® RCY6713 PC (Asia Pacific) Cycoloy* RCY6713 resin is an injection moldable high heat PC blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.5.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics GELOY HRA222 ASA GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. Use for exterior/interior electrical applications requiring UV resistance. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Asia Pacific) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXJ PC LNP* Lubricomp* DFL36XXJ is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180-1A |
Gromax BFG45-AS00N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, DRY Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical .. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4mm, Cut; ISO 180/1A |
SABIC Innovative Plastics SABIC STAMAX 20YK270 PP SABIC® STAMAX 20YK270 is a 20% long glass fiber reinforced polypropylene with improved impact and flow properties. The glass fibers are chemically coupled to the PP matrix, resulting in high stif.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, DRY Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Asia Pacific) PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 (Asia Pacific) LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP TH0815A LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180/1A |
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, Conditioned Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used.. |
|||
Izod Impact, Notched (ISO) | >= 17.0 kJ/m² | >= 8.09 ft-lb/in² | |
Styrolution Absolac® XT04M ABS High heatInformation provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP PF008 PA 6 (Asia Pacific) LNP THERMOCOMP* PF008 is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOTUF VF008 Super Tough Nylon LNP THERMOTUF* VF008 is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX0844 PPE+PS PPE+PS blend. Unfilled. UL94 HB rated. Low water absorption. Hydrolytic stability. Dimensional stability. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180 |
Polyram PlusTek RA303G50 Nylon 66 for Injection Molding, 50% Glass Fiber Reinforced, Heat Stabilized, Hydrolysis Resistant 50% Glass fiber reinforced, heat stabilized and hydrolysis resistant Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® 22LHI6 XE-NBK1 Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180 |
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180 |
Polyram RamTough PZ513 Polycarbonate, Easy Flow, Flame Retardant Transparent polycarbonate, UV stabilized, easy flow, flame retardant, for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180 |
Polyram PlusTek PD502G6 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced 30% Glass-fiber reinforced, V-0 1.6 mm, Nylon 12 for injection molding application.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-716 ABS - High Flow High flow, medium impact |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-765 ABS - Flame Retardant F.R. High Flow |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 1A; ISO 180 |
Azoty Tarnow™ TARNOFORM 300 CI4 POM Impact modified injection molding grade based on Tarnoform 300 reinforced with 20% MBS rubber yielding good cold impact strength and good strength of weld lines combined with good weatherability.Inf.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO Test |
BASF Ultramid® 1603-2 NF2004 43% Glass Filled PA66 (Conditioned) Ultramid 1603-2 NF2004 is a 43% glass reinforced, heat stabilized injection molding nylon 6/6 with the highest level of glass reinforcement for maximum strength and stiffness. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX2355 PPE+HIPS (Europe-Africa-Middle East) NORYL PX2355 is an unfilled, medium heat, low odour and low emission material with excellent heat aging performance. It has been developed for automotive interior applications, such as instrument pa.. |
|||
Izod Impact, Notched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B3WG5 BK 00564 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |