Category | Polymer , Thermoplastic , ASA Polymer , Polycarbonate (PC) , Polycarbonate/ASA Alloy, Unreinforced |
Manufacturer | SABIC Innovative Plastics (GE Plastics) |
Trade Name | GELOY |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | SABIC Innovative Plastics GELOY HRA222F ASA+PC (Asia Pacific).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
Moisture Absorption | 0.200 % | 0.200 % | 23°C / 50% RH; ISO 62 |
Water Absorption at Saturation | 0.60 % | 0.60 % | ISO 62 |
Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | on Tensile Bar; SABIC Method |
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 260 °C |
13 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 |
51.0 MPa | 7400 psi | 5 mm/min; ISO 527 | |
56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 | |
66.0 MPa | 9570 psi | Type I, 5 mm/min; ASTM D638 | |
Tensile Strength, Yield | 59.0 MPa | 8560 psi | Type I, 5 mm/min; ASTM D638 |
60.0 MPa | 8700 psi | 50 mm/min; ISO 527 | |
62.0 MPa | 8990 psi | 5 mm/min; ISO 527 | |
63.0 MPa | 9140 psi | Type I, 50 mm/min; ASTM D638 | |
Elongation at Break | >= 50 % | >= 50 % | 5 mm/min; ISO 527 |
>= 50 % | >= 50 % | 50 mm/min; ISO 527 | |
>= 100 % | >= 100 % | Type I, 50 mm/min; ASTM D638 | |
>= 100 % | >= 100 % | Type I, 5 mm/min; ASTM D638 | |
Elongation at Yield | 4.2 % | 4.2 % | Type I, 5 mm/min; ASTM D638 |
4.3 % | 4.3 % | 5 mm/min; ISO 527 | |
4.3 % | 4.3 % | Type I, 50 mm/min; ASTM D638 | |
4.4 % | 4.4 % | 50 mm/min; ISO 527 | |
Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 | |
Flexural Yield Strength | 93.0 MPa | 13500 psi | 2 mm/min; ISO 178 |
Flexural Modulus | 2.51 GPa | 364 ksi | 2 mm/min; ISO 178 |
Izod Impact, Notched | 3.85 J/cm | 7.21 ft-lb/in | ASTM D256 |
2.90 J/cm @Temperature 0.000 °C |
5.43 ft-lb/in @Temperature 32.0 °F |
ASTM D256 | |
Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
12.0 kJ/m² @Temperature 0.000 °C |
5.71 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A | |
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 69.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
38.3 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 | |
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
Deflection Temperature at 1.8 MPa (264 psi) | 88.0 °C | 190 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
Vicat Softening Point | 102 °C | 216 °F | Rate B/50; ISO 306 |
104 °C | 219 °F | Rate B/120; ISO 306 | |
111 °C | 232 °F | Rate A/50; ISO 306 | |
UL RTI, Electrical | 90.0 °C | 194 °F | UL 746B |
UL RTI, Mechanical with Impact | 90.0 °C | 194 °F | UL 746B |
UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
Flammability, UL94 | V-0 @Thickness 2.00 mm |
V-0 @Thickness 0.0787 in |
UL 94 |
Oxygen Index | 29 % | 29 % | ISO 4589 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | >= 600 V | >= 600 V | UL 746A |
600 V | 600 V | IEC 60112 |
Descriptive Properties | Value | Comments |
---|---|---|
Ball Pressure Test, 75°C +/- 2°C | PASSES | IEC 60695-10-2 |
UV-light, water exposure/immersion | F1 | UL 746C |