Polymer Property : Izod Impact, Unnotched (ISO) = 34.7 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 73.0 kJ/m²

@Temperature -30.0 °C
34.7 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® 505RU PC
Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro..
Izod Impact, Unnotched (ISO) 73.0 kJ/m²

@Temperature -30.0 °C
34.7 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific)
Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro..
Izod Impact, Unnotched (ISO) 73.0 kJ/m²

@Temperature -30.0 °C
34.7 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East)
Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE..
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP IFL36 PA6.12
LNP LUBRICOMP* IFL36 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP EX06430H PEI
LNP* THERMOCOMP* EX06430H is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this grade is: Healthcare.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES
LNP THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing 20% Glass Fiber.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Asia Pacific)
LNP* THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP JF004E PES (Asia Pacific)
LNP* Thermocomp* JF004E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES
LNP* THERMOCOMP* JF004EXP is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES (Asia Pacific)
LNP* Thermocomp* JF004EXP is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RX10408H PA 66
LNP* Thermocomp* RX10408H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP TH0815A
LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP TH0815A PUR (Asia Pacific)
LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA6.10
LNP THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA 6/10 (Asia Pacific)
LNP* THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²

@Temperature 23.0 °C
34.7 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Verton RV008ESV PA 66
40% long glass fiber filled PA66 Verton Xtreme XCThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²

@Temperature -30.0 °C
34.7 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1eU
Lubrizol ESTALOC® 59300 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Izod Impact, Unnotched (ISO) 73.0 kJ/m²

@Temperature 23.0 °C
34.7 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp TX88477 PU
LNP* Thermocomp* TX88447 is a compound based on Polyurethane resin containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP JF004E PES
LNP* THERMOCOMP* JF004E is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON PX00700 PA 6
LNP VERTON* PX00700 is a compound based on Nylon 6 resin containing proprietary fillers. Added feature of this grade is: Structural.
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON PX00700 PA 6 (Asia Pacific)
LNP* Verton* PX00700 is a compound based on Nylon 6 resin containing Long Glass Fiber.