Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 GF 15 TS PA66, 15% glass fibre FeaturesChemically reinforced with 15% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID® 6/66 GF 15 GB 15 PA6/66 reinforced with glass fiber, glass beads PA 6 and PA 66 alloy for injection molding, reinforced with 15% glass fiber and 15 % glass beads, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders .. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 93 T 20 PP, 20% mineral filling, UV stabilization FeaturesModified PP for injection moulding with the content of 20 % mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 20 Polyamide 6, 20% Glass Fiber FeaturesPA 6 for injection moulding, chemically coupled with 20% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and con.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-HGR24 Nylon 6-30% Glass Fiber and Glass Bead Reinforced (European Grade) (Dry)
(discontinued The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® KL 1-7265 000000 PBT, 15% Glass Fiber PBT, 15% glass fibers, injection molding |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® DP 2131/20 W1 901317 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, weather resistance, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eU |
Lanxess Pocan® A 3122 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXALEN PPH305G30 Polypropylene Homopolymer, 30% Glass Filled SAXALEN PPH305G30 is a 30% glass filled Polypropylene - Homopolymer injection molding grade with high stiffness, low creep under load and good flow properties.Information provided by SAX Polymers |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1fU |
Borealis Nepol™ GB601HP Polypropylene, 20% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis RA130E-6017 Polypropylene Random Copolymer RA130E-6017 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis RA130E-8427 Polypropylene Random Copolymer RA130E-8427 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is grey colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Polyram PlusTek PB340S50 Nylon 6 for Injection Molding, 50% Glass-beads Reinforced, Heat Stabilized 50% Glass-beads reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eU |
DSM Akulon® K222-KGV4 /A PA6-GF20 FR(30) 20% Glass Reinforced, Heat Stabilized, Flame Retardant (Halogen-phosphorous-free) |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K222-KWGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eU |
DSM Stanyl® TW241B3 PA46-CF15 15% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
Eurotec® Tecodur® PB70 NL XA 20 PBT unreinforced, UL94 V0 Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
Eurotec® Tecomid® NA40 NL FA 50 PA 6.6 unreinforced, UL94 V0, halogen/phosphorus free Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eU |
DSM Akulon® K224-G3-FC NA99001 PA6-GF15 15% Glass Reinforced |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM EcoPaXX® Q-KGS6 PA410-GF30 FR 30% Glass Reinforced, Flame Retardant (Halogen free) |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eU |
Barlog Plastics KEBATER BF110 PBT, 10% glass fiber reinforced PBT-GF10Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 NG GF 20 PA6, 20% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVASTER® B GF 20 FRL 4 Polybutylene Terephthalate, 20% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant FeaturesPBT with the content of 20% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S CV300 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |