Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 17.9 MPa | 2600 psi | 2 in/min; ASTM D638 |
RheTech Products FT1001-177UV Thermoplastic Polyolefin, Non-UV Stabilized, HS5 Medium Dark Neutral Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | 2 in/min; ASTM D638 |
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | 2 in/min; ASTM D638 |
RheTech Products FT3080-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | 2 in/min; ASTM D638 |
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | 2 in/min; ASTM D638 |
RheTech Products FT3080-727UV Thermoplastic Polyolefin, UV Stabilized, G01 Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | 2 in/min; ASTM D638 |
RheTech Products FT3080-81 Thermoplastic Polyolefin, UV Stabilized, ACRA Titanium Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | 2 in/min; ASTM D638 |
RheTech Products FT4802-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | 2 in/min; ASTM D638 |
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | 2 in/min; ASTM D638 |
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.9 MPa @Temperature 23.0 °C |
2600 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE) OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.Purge thoroughly before and af.. |
|||
Tensile Strength at Break | >= 17.9 MPa | >= 2600 psi | ASTM D638 |
S&E Specialty Polymers GPP6100-116C PP Application: Specially engineered, low bloom, low specific gravity, flame retardant polypropylene compound designed with halogen based technology. Exhibits a unique balance of high flexural modulus .. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | |
NEU Neuthane N8511-1H Aromatic, Polyester TPU Blend A blend of aromatic, polyester TPUs with good clarity |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D1414 |
Greene Tweed FLUORAZ® 890 Fluoroelastomer, FEPM Sanitary gaskets made from Fluoraz® 890 are ideal for use in standard SIP and CIP applications where EPDMs and FKMs fail. While EDPMs and FKMs can provide a deal for extended periods, changes in.. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D412 |
ITW Devcon Rubber Repair / Castable Urethane Cable Cast FR, Black Information provided by ITW Devcon |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D638 |
Teknor Apex APEX® 84842 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; High Heat Resistance; Sunlight Resistant (720 hours); RoHS Compliant Forms: Pellets Uses: Cable Jacketing; Outdoor Applications Wire Types: CXTW; SPT-1W; STW; XTW; SJTW; .. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D638 |
Teknor Apex APEX® 85-J644Z-3 Polyvinyl Chloride, Flexible Notes: 105°C Jacket Forms: Pellets Agency Ratings: UL 13; UL 1424; UL 1655; UL 2250; UL 444 Wire Types: CATV; CL3; CMX; CL2; CM; FT-4Information Provided by Teknor Apex |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D638 |
Teknor Apex Flexalloy® 89501-83 Polyvinyl Chloride, Elastomer Notes: 105°C Insulation; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility Uses Wet Rated Insulation Wire Types: NISPE-1; NISPE-2; SE; SEO; SEOW; SEW; SJ.. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D412 |
Teknor Apex Monprene® MP-1538A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D412 |
Teknor Apex Monprene® MP-1878B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D638 |
Teknor Apex Fireguard® 910-A10-NL2 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant; Low Smoke Emission Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 800;.. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D412 |
Teknor Apex Telcar® TL-1446G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D412 |
UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | at 2.0 in/min, Tested using a 50 mil. Sheet; ASTM D638 |
Chevron Phillips EB6755 Rubber Modified Polystyrene DescriptionChevron EB6755 is an extrusion grade, high impact polystyrene developed for use in packaging applications. It is designed for exceptional environmental stress-crack resistance and practi.. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | vs. aluminum; 130 s set time |
Elmer's Products Aron Alpha® 203 Cyanoacrylate Adhesive (Industrial Krazy Glue™) General purpose adhesive for a variety of applications. Various viscosities and gap filling properties available.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair o.. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D412 |
Compuestos Dominicanos Polycom VY-050775 PVC Compound The Polycom VY series are compounds for the extrusion of both stripes for chaise lounge and flexible window sidings with outstanding weather and outdoes resistance. Also, in the VY series the are p.. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | Press cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 232°C; ASTM D412 |
3M Dyneon™ PFE 60Z Perfluoroelastomer Dyneon™ PFE 60 Z is a technically advanced peroxide curable perfluoroelastomer, designed to meet the challenges of demanding sealing applications. It’s fully fluorinated back bone structure provid.. |
|||
Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D638 |
ExxonMobil Paxon™ AG45-004 Blow Molding Resin
(discontinued **) AG45-004 is a blow molding high density polyethylene which offers exceptional stress crack resistance and impact performance. It contains an antistat which permits this resin to be used in all food.. |