Teknor Apex APEX® 85-J644Z-3 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 85-J644Z-3 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: 105°C Jacket Forms: Pellets Agency Ratings: UL 13; UL 1424; UL 1655; UL 2250; UL 444 Wire Types: CATV; CL3; CMX; CL2; CM; FT-4Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
15 seconds; ASTM D2240
Tensile Strength at Break 17.9 MPa
2600 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous Use; ASTM D794
Brittleness Temperature -29.0 °C
-20.2 °F
ASTM D746
Oxygen Index 31 %
31 %
ASTM D2863
Descriptive Properties Value Comments
Appearance Opaque