Mechanical Properties Metric English Comments
Tensile Strength at Break 174 MPa
25200 psi
50 mm/min; ISO 527-1,2
Qualchem Danamid FCF-20 Polyamide 6, 20% Carbon Fiber
Reinforced with carbon fiber, antistatic and conductive.Information provided by Qualchem Zrt.
Tensile Strength at Break 174 MPa
25200 psi
ASTM D638
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Tensile Strength at Break 174 MPa
25200 psi
ISO 527 Type 1A
Solvay TECHNYL® A 218G V33 Black 41N PA66, 33% glass fiber, DRY
Description: TECHNYL® A 218G V33 Black 41N is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This pr..
Tensile Strength at Break 174 MPa
25200 psi
ASTM D 638
SABIC Innovative Plastics LNP Lubricomp ICP36 PA 6/12 (Asia Pacific)
LNP* Lubricomp* ICP36 is a compound based on Nylon 6/12 resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conductive.This data was ..
Tensile Strength at Break 174 MPa
25200 psi
ASTM D 638
SABIC Innovative Plastics LNP Lubricomp ICP36 PA6.12
LNP* Lubricomp* ICP36 is a compound based on Nylon 6/12 resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conductive.This data was ..
Tensile Strength at Break 174 MPa
25200 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP OCL36EXP PPS - LINEAR
LNP* LUBRICOMP* OCL36EXP is a compound based on Linear PPS containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include; Wear Resistant, Electrically Conductive.
Tensile Strength at Break 174 MPa
25200 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RFP38 PA6.6
LNP* LUBRICOMP* RFP38 is a compound based on Nylon 66 containing 40% Glass Fiber, 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
Tensile Strength at Break 174 MPa
25200 psi
ASTM D638
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry)
Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Tensile Strength at Break 174 MPa
25200 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF0069SF PA 66
LNP* THERMOCOMP* RF0069SF is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Tensile Strength at Break 174 MPa
25200 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF0069SF PA 66 (Asia Pacific)
LNP* Thermocomp* RF0069SF is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
Tensile Strength at Break 174 MPa
25200 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON EX07311P PEI (Asia Pacific)
LNP Stat-kon* EX07311P is an easy flowing ESD-safe compound based on Polyetherimide resin. This compound is developed for good dimensional stability for use in ESD Tray for Backend Semicon and HDD t..
Tensile Strength at Break 174 MPa
25200 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP EF006E PEI
LNP THERMOCOMP* EF006E is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
Tensile Strength at Break 174 MPa
25200 psi
ISO 527-2
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Tensile Strength at Break 174 MPa
25200 psi
ISO 527-2
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Tensile Strength at Break 174 MPa
25200 psi
ISO 527-2
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Tensile Strength at Break 174 MPa
25200 psi
ISO 527-2
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded
Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe..
Tensile Strength at Break 174 MPa
25200 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Verton PV007SV_YW8D151 PA 6
Preliminary data for 35% long fiber single pellet color filled PA6This data was supplied by SABIC-IP for the Americas region.
Tensile Strength at Break 174 MPa
25200 psi
Type I, 5 mm/min; ASTM D638
LNP ULTEM® SMU5834 Polyetherimide, 20% Carbon Fiber Reinforcement  (discontinued **)
High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo..
Tensile Strength at Break 174 MPa
25200 psi
ISO 527-2
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Tensile Strength at Break 174 MPa
25200 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOTUF IX02582 PA 6/12 (Asia Pacific)
LNP* Thermotuf* IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact.
Copyright © lookpolymers.com All Rights Reserved