Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 120 MPa | 17400 psi | |
Plastcom SLOVAMID 6 GF 30 FRA 3 PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 850°C,.. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | ISO 527-2 |
PolyOne OnForce™ LFT PP-40LGF/001 UV Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Strength at Break | <= 120 MPa | <= 17400 psi | 50 mm/min; ISO 527-1,2 |
Qualchem Danamid FGF-15 Polyamide 6, 15% Glass Fiber Reinforced with glass fiber.Information provided by Qualchem Zrt. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | ASTM D638 |
Ravago Manufacturing Americas Hylex® P1010G30FRMA Polycarbonate, 30% Glass Filled Polycarbonate, 30% Glass Filled, Flame RetardantInformation provided by Ravago. |
|||
Tensile Strength at Break | 120 MPa @Temperature 23.0 °C |
17400 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® APTIV® 2102-050 Polyetheretherketone (PEEK) Polymer Film, Amorphous, Mineral Filled
(discontinued ** APTIV PEEK 2100 series films are the mineral filled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTIV.. |
|||
Tensile Strength at Break | 120 - 140 MPa | 17400 - 20300 psi | ASTM D683 |
Loxim 230 12V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | ISO 527-1, -2; 5 mm/min |
Lanxess Pocan® ECO T 3220 000000 PBT + PET, 20% Glass Fiber PBT + PET, 20% glass fibers, injection molding, improved surface finish, contains 28% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | ISO 527 |
Solvay TECHNYL® C 218L V30 PA6, 30% glass fiber, Eh 50 Description: TECHNYL C 218 L V30 is a polyamide 6 reinforced with 30% glass fiber and UV stabilized.Colors: it is marketed in the natural and black color.Available in: Latin America Main Properties:.. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3240A PP SABIC® PPcompound G3240A is a general purpose, 40% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 139448304. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 420SE0 PBT 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 420SE0U PBT PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® K4560 PBT (Europe-Africa-Middle East) 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | ISO 527 |
SABIC Innovative Plastics LNP Thermocomp DF0069E PC (Asia Pacific) LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC.. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | 50mm/min; ISO 527 |
Teijin Panlite® BS-8120R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact.. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | ISO 527-1/-2 |
DSM Akulon® K224-HGM35 (Dry) 15% Glass Reinforced, 25% Mineral Reinforced, Heat Stabilized Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MX 400 CP Combination Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MZ 301 CP Combination Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-30H FWA nat PA12-GF30 Product description: Grilamid LV-30H FWA natural is a 30 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G25HSLR BK099 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR BK099 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | ISO R 527 |
Addiplast Addinyl B2 G10 V20 Nylon 6, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
Tensile Strength at Break | 120 MPa @Temperature 150 - 160 °C, Time 1.80e+7 sec |
17400 psi @Temperature 302 - 320 °F, Time 5000 hour |
5 [mm/min], 50% Loss of Tensile Strength; ICE 216 |
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Strength at Break | 120 MPa | 17400 psi | ASTM D638 |
Beijing Chemical Industry KAIFA® 301-G30 PBT Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |