Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® C 218L V30 PA6, 30% glass fiber, Eh 50

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 218L V30 PA6, 30% glass fiber, Eh 50.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: TECHNYL C 218 L V30 is a polyamide 6 reinforced with 30% glass fiber and UV stabilized.Colors: it is marketed in the natural and black color.Available in: Latin America Main Properties: ? Excellent superficial aspect, Excellent dimensional stability, Good thermal resistance,? UV stabilization and Good impact resistance Applications: TECHNYL C 218 L V30 was developed for applications where good balance of mechanical and thermal properties are required with good superficial aspect.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
ISO 527
Elongation at Break 4.5 %
4.5 %
ISO 527
Tensile Modulus 6.20 GPa
899 ksi
ISO 527
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
CEI 93
Dielectric Constant 4.5
4.5
CEI 250
Dielectric Strength 22.0 kV/mm
559 kV/in
CEI 93
Dissipation Factor 0.0090
0.0090
CEI 250
Comparative Tracking Index 475 V
475 V
CEI 112