| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled , Polybutylene Terephthalate (PBT), Flame Retardant |
| Manufacturer | Loxim Industries |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Loxim 230 12V0 Polybutylene Terephthalate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.65 - 1.70 g/cc | 1.65 - 1.70 g/cc | ASTM D792 |
| Filler Content | 30 % | 30 % | |
| Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D1299 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 120 - 140 MPa | 17400 - 20300 psi | ASTM D683 |
| Elongation at Break | 2.0 % | 2.0 % | ASTM D638 |
| Tensile Modulus | 9.00 GPa | 1310 ksi | ASTM D638 |
| Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
| Izod Impact, Notched | 0.650 - 0.750 J/cm | 1.22 - 1.41 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 210 - 215 °C | 410 - 419 °F | ASTM D1525, HDT Method B |
| Flammability, UL94 | V-0 @Thickness 1.60 mm |
V-0 @Thickness 0.0630 in |