Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 115 MPa | 16700 psi | |
Plastcom SLOVAMID 66 GF 15 TS PA66, 15% glass fibre FeaturesChemically reinforced with 15% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527-1/-2 |
DSM Akulon® K224-HGR24 Nylon 6-30% Glass Fiber and Glass Bead Reinforced (European Grade) (Dry)
(discontinued The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527-1/-2 |
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | |
LATI Latilub 57-30GRTS G/20 PPA, 20% Glass Fiber Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | |
LATI Latiohm 87/26-06 PD01-V1 PC, Flame Retardant Semiconductive/dissipative product based on Polycarbonate (PC). UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2100R PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM PW2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified... |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® K4560 PBT (Europe-Africa-Middle East) 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU LNP* THERMOCOMP* GX05482 is a compound based on Polysulfone resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, Conditioned Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co.. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem LTX931A PEI Blend (Europe-Africa-Middle East) Post-industrial recycle based, 30% glass fiber filled, high flow Polyetherimide blend. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ASTM D638 |
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527-2 |
Tisan TISESTER® 15% Glass Fiber Reinforced and Heat Stabilized Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527-2 |
Tisan TISESTER® 15% Glass Fiber Reinforced Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527-1/-2 |
DSM Stanyl® 46HF4130 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527-1/-2 |
DSM Stanyl® TW200F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4106 nat PA612-GF30 Product description: Grilamid XE 4106 natural is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorptiong.. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® LW9320LM BK591 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320LM is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. It ha.. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK692FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK692FR is a 15% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided by .. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527 |
Eurotec® Tecotek® PC40 GR20 NL PC, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527-2/5 |
Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Conditioned, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Tensile Strength at Break | 115 MPa @Temperature 160 - 175 °C, Time 1.80e+7 sec |
16700 psi @Temperature 320 - 347 °F, Time 5000 hour |
5 [mm/min], 50% Loss of Tensile Strength; ICE 216 |
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL BK039 is a 13 % glass reinforced heat stabilized lubricated slightly toughened black polyamide 66 for injection molding. It.. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
Tensile Strength at Break | 115 MPa | 16700 psi | ISO 527-1/-2 |
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |