Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 26.0 MPa | 3770 psi | ISO.527 DIN.53455 |
Omnia Plastica PE 500 - Polyethylene 500 Polyethylene with a molecular weight of ± 500,000. PE 500 is more rigid than the high molecular weight polyethylene and it is therefore more suitable for mechanical applications. The friction coeff.. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | 2 in/min; ASTM D638 |
RheTech Products HP531-01UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: IP structural componentsAir ducts - distributionA/B/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | 2 in/min; ASTM D638 |
RheTech Products HP531-678UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, IT3A Medium Light Stone Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | <= 26.0 MPa | <= 3770 psi | ISO/R527 |
Polykemi AB POLYfill PP EIP12030RF Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
Tensile Strength at Break | 26.0 - 28.0 MPa | 3770 - 4060 psi | ASTM D683 |
Loxim 821 02T HB Polypropylene Compound, 20% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Tensile Strength at Break | 26.0 - 28.0 MPa | 3770 - 4060 psi | ASTM D683 |
Loxim 840 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | after 7days @136°C; UL 1581 |
SABIC Innovative Plastics NORYL WCA875 PPE-TPE Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t.. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | UL 1581 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | UL 1581 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Asia Pacific) Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Tensile Strength at Break | >= 26.0 MPa | >= 3770 psi | ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® HX3061HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity: 250C at 21.6 kgf is 1450-1850 poise. Available in Natural color (1001) only. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON MD000A PP LNP* STAT-KON* MD000A is a compound based on Polypropylene resin containing Carbon. Added feature of this grade is: Electrically Conductive. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | ASTM D638 |
SCG Chemicals EL-Leneâ„¢ H5480S High Density Polyethylene Monofilament Key Characteristics:High tenacityExcellent product colorRecommended Applications: Monofilament and flat yarn extrusion for manufacturing of nets, ropes and tarpaulinInformation provided by SCG Chem.. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | ISO 527-2 |
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | ISO 527-1/-2 |
Covestro Desmopan® W DP 85786A Polyurethane Grade for calanderingno yellowing under the action of UV lightgood low-temperature flexibilityhigh rebound resilienceimproved microbial resistanceImproved hydrolysis resistanceApplicationTextile coa.. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | ISO 527-2/50 |
ExxonMobil Exxtral™ HMU 216 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by high stiffness and designed for automotive exterior applications in which good surface finish and good UV resistance .. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® PC945 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | ASTM-D638 |
Braskem IA58 HDPE Injection Molding Polyethylene Copolymer IA58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers good processability combined with good .. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | ASTM-D638 |
Braskem IB58 HDPE Injection Molding Polyethylene Copolymer IB58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers good processability combined with good .. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0339W10L1 Wollastonite Reinforced |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0339W40L1 Wollastonite Reinforced |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | ISO 527 |
Breplast Bretene PP Polypropylene Composite Recovered polypropylene compositeInformation provided by Breplast S.p.A. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | Conditioned; ISO R 527 |
Addiplast Addilene J 490 M20S Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | ISO R 527 |
Addiplast Addilene PMD 50245 Polypropylene Homopolymer For electroplatingInformation provided by Addiplast. |
|||
Tensile Strength at Break | >= 26.0 MPa | >= 3770 psi | ASTM D4745-11 |
Adamas Adalon® 503 PTFE, 0.1% MoS2 Information provided by Adamas, HPM |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | |
3M Dyneon™ PFA 6515NZ Perfluoroalkoxy Fluorothermoplastic PFA designed for higher speed or higher shear processing such as injection molding and wire insulation. Demonstrates universal chemical and solvent resistance, high dielectric strength, excellent we.. |
|||
Tensile Strength at Break | >= 26.0 MPa @Temperature 23.0 °C |
>= 3770 psi @Temperature 73.4 °F |
ASTM D1708 |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, .. |
|||
Tensile Strength at Break | >= 26.0 MPa @Temperature 23.0 °C |
>= 3770 psi @Temperature 73.4 °F |
ASTM D1708 |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Tensile Strength at Break | 26.0 MPa | 3770 psi | ASTM D638 |
Toyobo PELPRENE™ P48U Polyester TPE, Weather-resistant Features: Polyester TPE, Weather-resistantInformation provided by Toyobo. |
|||
Tensile Strength at Break | >= 26.0 MPa @Strain >=100 % |
>= 3770 psi @Strain >=100 % |
ISO R527 |
Shanghai Ofluorine 9201 PVDF Pellets for cables Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, .. |