Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
5.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D4812 |
PolyOne Geon™ 81530 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Unnotched | 2.70 J/cm @Temperature 23.0 °C |
5.06 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
PolyOne Edgetek® AS-10GF/000 FR V0 BLACK Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Izod Impact, Unnotched | 2.70 - 5.23 J/cm | 5.06 - 9.80 ft-lb/in | Average value: 3.71 J/cm Grade Count:3 |
Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
Izod Impact, Unnotched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ryton® R-4 02 Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4 02 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at elev.. |
|||
Izod Impact, Unnotched | >= 2.70 J/cm | >= 5.06 ft-lb/in | ASTM D256 |
Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE Namtene® 1002 is used for pipes. It features a lower polypropylene content than standard Namtene®. |
|||
Izod Impact, Unnotched | >= 2.70 J/cm | >= 5.06 ft-lb/in | ASTM D256 |
Forever Plast Namtene® Recycled Standard HDPE Standard Namtene® is used for dimple sheet, plastic slabs, and agricultural and construction applications. |
|||
Izod Impact, Unnotched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 2030 Polyarylamide (PARA), 55% GlassMineral Ixef® 2030 is a 55% glass-fiber/mineral reinforced polyarylamide compound which exhibits high strength, very high stiffness, low warpage, excellent creep resistance and outstanding surface gloss... |
|||
Izod Impact, Unnotched | 2.70 J/cm @Thickness 3.18 mm |
5.06 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs.. |
|||
Izod Impact, Unnotched | 2.70 J/cm @Thickness 3.18 mm |
5.06 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S.. |
|||
Izod Impact, Unnotched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI) Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w.. |
|||
Izod Impact, Unnotched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Adell EQ-14 Homopolymer Polypropylene, 20% Mica Filled Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Adell RQ-16 Copolymer Polypropylene, 30% Mica Reinforced Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Chevron Phillips Ryton® R-7 02 Polyphenylene Sulfide Compound
(discontinued **) Black Polyphenylene Sulfide CompoundRyton® R-7 02 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compound wit.. |
|||
Izod Impact, Unnotched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON LX00797C PEEK LNP* STAT-KON* LX00797C is a compound based on Polyetheretherketone containing Proprietary Filler(s). Added features of this material include: ristics of this grade are: Clean Compounding System, .. |