Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.00 - 2.00 J/cm² | 4.76 - 9.52 ft-lb/in² | ISO 11542-2 |
Okulen® 500 PE-HMW, AST OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Charpy Impact Unnotched | 1.00 - 2.00 J/cm² | 4.76 - 9.52 ft-lb/in² | ISO 11542-2 |
Okulen® 500 PE-HMW, Coloured OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Charpy Impact Unnotched | 1.00 - 1.30 J/cm² | 4.76 - 6.19 ft-lb/in² | ISO 11542-2 |
Okulen® 1000 - REG PE Multicoloured fine OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data, Low Temp |
Americas Styrenics Styron® 663 Polystyrene
(discontinued **) STYRON® 663 general purpose polystyrene resin is an additive free resin with excellent strength, clarity, and high heat resistance. When used unmodified for the manufacture of food contact articles.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data, Low Temp |
Americas Styrenics Styron® 685P Polystyrene
(discontinued **) STYRON® 685P general purpose polystyrene resin is a high heat resin with good strength, moldability/processability, and excellent clarity. This resin is typically used in consumer electronic applic.. |
|||
Charpy Impact Unnotched | 1.00 - 5.00 J/cm² | 4.76 - 23.8 ft-lb/in² | Average value: 2.69 J/cm² Grade Count:7 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
Polimeri Europa EDISTIR N1670 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,095-06 General purpose polystyrene with good flow and good heat resistance. Recommended for extrusion in blend with HIP.. |
|||
Charpy Impact Unnotched | 1.00 - 4.00 J/cm² | 4.76 - 19.0 ft-lb/in² | Average value: 3.00 J/cm² Grade Count:38 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² - NB | 4.76 ft-lb/in² - NB | Average value: 3.77 J/cm² Grade Count:30 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 6506 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures, UL Listed
&nbs Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant, UL listed molding compound 1.5 mm/V-.. |
|||
Charpy Impact Unnotched | 1.00 - 4.40 J/cm² | 4.76 - 20.9 ft-lb/in² | Average value: 2.14 J/cm² Grade Count:20 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1301-7508 PPS, linear, with glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1301-7836 PPS, linear, with glass fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts.High dim.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1301-8306 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Lastil G/25-V0 SAN, 25% Glass Fiber Reinforced, Flame Retardant Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants. Very high dimensional stability.Availability: Africa & Middle East; Asia Pa.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Latamid 12 CP/85 PA 12 Polyamide 12 (PA12) based compound. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Latishield 36/AR-10A-V0E ABS, Steel Fiber Reinforced, Flame Retardant EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Information provided by Lati Indust.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
Styrolution NOVODUR® P2MC ABS, Injection Grade Injection molding grade for plating; very good ratio between toughness, heat resistance and flow.Applications: All parts to plating: e.g. sanitary parts. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179 |
Vyncolit X689 Novolac Phenolic Glass fiber filled and molybdeendisulfide modified phenolic molding compound with excellent mechanical and thermal properties and lower thermal expansion coefficient. It has excellent friction prop.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® HT KU 1-9331 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Lighting, automotive and household goods, light covers, indicator and brake light lenses.Information provided by Bayer.As of 1 September 2015, Ba.. |
|||
Charpy Impact Unnotched | >= 1.00 J/cm² | >= 4.76 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.2 |
Hippe PF WV 201 Wood veneer Reinforced Phenolic Resin - Sheet Cross plied. Used in mechanical applications. Good mechanical properties.Information provided by Hippe. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data |
Dow Tyril® 125 SAN Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data, Low Temp |
Dow Tyril® 125 SAN Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data |
Dow Tyril® 990 SAN TYRIL® 990 SAN copolymer grade provides colorless glass-like clarity and excellent overall optical properties. It provides a profile of very good strength with stiffness, chemical resistance, heat .. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data |
Dow Tyril® 1000B SAN TYRIL® 1000B SAN copolymer offers the best balance of physical properties of all TYRIL grades. It also provides excellent processability and chemical resistance, superior heat resistance, and good .. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® D 1189 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.00 - 1.50 J/cm² | 4.76 - 7.14 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RALUPOL® 8605 UP Polyester Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire.. |
|||
Charpy Impact Unnotched | 1.00 - 4.90 J/cm² | 4.76 - 23.3 ft-lb/in² | Average value: 3.37 J/cm² Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Charpy Impact Unnotched | 1.00 - 7.20 J/cm² @Temperature -40.0 - -20.0 °C |
4.76 - 34.3 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.07 J/cm² Grade Count:2 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |