Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | DIN 53453 |
Nilit FRIANYL C73 H-GV15 Nylon 6.6/6 for injection molding, 15% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 4.50 - 6.00 J/cm² @Temperature -30.0 - -30.0 °C |
21.4 - 28.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.25 J/cm² Grade Count:2 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -40.0 °C |
21.4 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 4.50 J/cm² - NB | 21.4 ft-lb/in² - NB | Average value: 8.27 J/cm² Grade Count:27 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 50-7164/BL02 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Low warpag.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 80/TF/22/NT Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | |
Idemitsu Kosan Xarec® WA 212LG SPS, 30% Glass Filled |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 1-1108 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-7943 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 420HP PBT 30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179 |
Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Dry) Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.Information provided by STYROLUTION, which is a join.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179-1 |
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Dry Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 30.0 °C |
21.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-15 S PA6-GF15 Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GV 10 HWCP 10% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® TSM-30 PA666-MD30 Product description: Grilon TSM-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral. Grilon TSM-30 has the following important properties: Excellent surface.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide BG3 PA6, 15% Glass Filled, Injection Molded BG3 is a 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179 1eU |
Azoty Tarnow™ Tarnamid® T-27 MK30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl A2 M20 V10 Nylon 66, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 1-7233-1 Polyamide 66, with glass fiber, PTFE, lubricant modified, silicone-free Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |
|||
Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179/1eU |
Borealis Daplen™ KB4436 TPO Compound Daplen KB4436 is a 30% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen KB4436 is a material with excellent impact/stiffness ratio. Thanks to its low the.. |
|||
Charpy Impact Unnotched | 4.50 J/cm² @Temperature -20.0 °C |
21.4 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Daplen™ KB4436 TPO Compound Daplen KB4436 is a 30% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen KB4436 is a material with excellent impact/stiffness ratio. Thanks to its low the.. |