Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -40.0 °C |
19.0 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 HS-GV40 Nylon 6.6 for injection molding, 40% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 4.00 - 4.00 J/cm² @Temperature -30.0 - -30.0 °C |
19.0 - 19.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.00 J/cm² Grade Count:2 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-7916 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1301-7662/BK PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1700-8541 PPO, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Isotropic shrinkage characteristics.Superheated steam sterilizable.Infor.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 2205-7054 Blend based on polyaryl ether ketone, with glass fiber Applications: High dimensionally stable precision parts, high continuous use temperature.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceChemical and hydr.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 50-7110 Polycarbonate, with carbon fiber, low-warpage, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Electrically conductive, suitable for continuous discharging o.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-0699-1 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | |
LATI Latilub 66-20T G/20 PA66, 20% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | |
LATI Latistat 66-06 G/30 PA66, 30% Glass Fiber Reinforced Dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics ULTEM HU2400 PEI (Asia Pacific) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East) VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East) VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 30.0 °C |
19.0 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-15/2 PA6-GF15 Product description: Grilon BG-15/2 is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15/2 has the following important properties: Good surface finishEasy processingG.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-25 HM PA6-GF25 Product description: Grilon BG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 25% glass fibers. Grilon BG-25 HM has the following important prop.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 30.0 °C |
19.0 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-30 FR PA6-GF30 FR Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 30.0 °C |
19.0 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HT XE 3996 PA*-GF30 Product description: Grivory XE 3996 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO-Polymer designatio.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 30.0 °C |
19.0 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-50 HM PA6-GF50 Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179-1eU |
Barlog Plastics KEBATRON L1040G3 PPS, linear, 40% glass fiber reinforced PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179/1eU |
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179/IeU |
Addiplast Addilene J 220 M40 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® 301-G15F PBT Resin 15% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | |
LATI Latiohm 66-04 PD01 G/25-V0CT1 PA66, 25% Glass Fiber Reinforced, Flame Retardant Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific;.. |