Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.80 J/cm² @Temperature -30.0 °C |
18.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Nilit FRIANYL A63 GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | ISO 179/1eU |
Nilit FRIANYL A63 HH-KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 HS-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 H-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | ISO 179/1eU |
Nilit FRIANYL B63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | ISO 179/1eU |
Nilit FRIANYL B63 FK 1010 Nylon 6 for injection molding, 10% glass fiber and 10% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.80 J/cm² @Temperature -40.0 °C |
18.1 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 H-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.80 - 1000 J/cm² | 18.1 - 4760 ft-lb/in² | Average value: 4.90 J/cm² Grade Count:6 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² - NB | 18.1 ft-lb/in² - NB | Average value: 8.46 J/cm² Grade Count:171 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Charpy Impact Unnotched | 3.80 - 17.0 J/cm² | 18.1 - 80.9 ft-lb/in² | Average value: 10.1 J/cm² Grade Count:6 |
Overview of materials for Nylon 12, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 19-7312/GN Polyamide 46, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 19-7969 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 19-8073 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1106-8133 Polyether imide, with carbon fiber, easy flowing Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific) LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² @Temperature -30.0 °C |
18.1 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Europe-Africa-Middle East) PPX7110 is an alloy of PP and PPO, providing high impact and good heat resistance. Generic identification acc. ISO11469: >PP+PPE+PS-I |
|||
Charpy Impact Unnotched | 3.80 J/cm² @Temperature 23.0 °C |
18.1 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Novamid® 1010G30 NA PA6-GF30 30% Glass Reinforced, Injection Molding, Easy Molding Grade, High Flow |
|||
Charpy Impact Unnotched | 3.80 J/cm² @Temperature 23.0 °C |
18.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 CF20 HWCP 20% Carbon Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTNFG52G35HSL BK011 is a 35% glass reinforced lubricated heat stabilized high performance polyamide resin developed for consideration into a.. |
|||
Charpy Impact Unnotched | 3.80 - 3.80 J/cm² @Temperature -20.0 - -20.0 °C |
18.1 - 18.1 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 3.80 J/cm² Grade Count:1 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | |
LATI Latilub 88/10-15T G/30 PEEK, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Charpy Impact Unnotched | 3.80 J/cm² | 18.1 ft-lb/in² | ISO 179/IeU |
Addiplast Addilene J 326 V30 Polypropylene Copolymer High modulus, high durabilityInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 3.80 - 3.80 J/cm² @Temperature -30.0 - -30.0 °C |
18.1 - 18.1 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.80 J/cm² Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |